MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 10-5/AboCure 3-4 Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 3-4 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 3-4 is a tan room-temperature-cure converter in paste form. AboCast 10-5/AboCure 3-4 is used as a thick adhesive for metal, ceramic, glass, and other rigid materials, or also for troweling rustproof wear resistant surfaces. It offers good thermal conductivity. As AboCure 3-4 can be used from 25 to 70 pbw with 100 pbw AboCast 10-5, the properties of the cured product can vary from the higher rigidity and chemical and heat resistance of the lower AboCure ratios (25-30 pbw) to the higher flexibility, thermoshock resistance, and better adhesion to critical substrates of the higher AboCure ratios (up to 60-70 pbw). This blend's main advantages are: it has variable ratios and is very thick, slow, room-temperature-cure, adhesive, and thermocycling. It also is dielectric and offers good adhesion, virtually no shrinkage, and high resistance to alkalis, diluted acids, water, many solvents, and outdoors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 60 min
@Temperature 25.0 °C
60 min
@Temperature 77.0 °F
100 g
 
Descriptive Properties
ColorGreen
Hardening Time (min)120 to 36025°C
Parts by Weight (pbw)100AboCast 10-5
 25-70AboCure 3-4
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Unreinforced
Abatron AboCast 10-5/AboCure 50-12 Epoxy
Abatron AboCast 10-5/AboCure 50-3 Epoxy
Overview of materials for Epoxy Adhesive, Flexible
Overview of materials for Epoxy, Molded, Glass Fiber Filler

PABC801 / 107785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.