MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded
Categories: Polymer; Thermoset; Melamine; Melamine-Phenolic Copolymer; Phenolic

Material Notes: PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E40654. 00714 is available in brown.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ASTM D1895
Density 1.67 g/cc0.0603 lb/in³ASTM D792
Water Absorption 0.275 %0.275 %ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7676ASTM D785
Tensile Strength, Ultimate 57.0 MPa8270 psiASTM D638
Elongation at Break 0.57 %0.57 %ASTM D638
Tensile Modulus 11.8 GPa1710 ksiASTM D638
Flexural Strength 97.0 MPa14100 psiASTM D790
Flexural Modulus 9.80 GPa1420 ksiASTM D790
Compressive Strength 164 MPa23800 psiASTM D695
Izod Impact, Notched 0.162 J/cm0.303 ft-lb/inASTM D256
Charpy Impact, Notched 0.199 J/cm²0.947 ft-lb/in²ASTM D256
Impact 8181J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D247
Dielectric Constant 7.07.0ASTM D150
Dielectric Strength 6.60 kV/mm168 kV/inStep by Step; ASTM D149
 9.30 kV/mm236 kV/inShort Time; ASTM D149
Dissipation Factor 0.0620.062ASTM D150
Arc Resistance 186 sec186 secASTM D495
Comparative Tracking Index 475 V475 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.580 W/m-K
@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 152 °C306 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 202 °C396 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 36 %36 %ASTM D2863
Shrinkage 0.69 %0.69 %240 hr, 105ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ 91G60 Polyamide 66, MF Reinforced
Addiplast Addinyl PMD 20164 Nylon 6
Norplex-Micarta NP509 Melamine Glass Laminate Sheet, NEMA G-5
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet
Gromax Melamine

PLEL01 / 50569

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.