MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 7021 Black Impact Grade Phenolic Molding Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Impact Grade, Filled

Material Notes: Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of switchgear parts, or where mechanical assembly requires better impact strength.

Data provided by Plaslok Corporation.

Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ASTM D792
Apparent Bulk Density 0.480 g/cc0.0173 lb/in³ASTM D1895
Water Absorption 0.50 %0.50 %ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inCompression; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.0 MPa5950 psiASTM D638
Flexural Yield Strength 74.0 MPa10700 psiASTM D790
Flexural Modulus 6.90 GPa1000 ksiASTM D790
Compressive Yield Strength 228 MPa33100 psiASTM D695
Izod Impact, Notched 0.240 J/cm0.450 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 6.00e+9 ohm-cm6.00e+9 ohm-cmASTM D257
Dielectric Constant  4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
ASTM D150
 6.0
@Frequency 60 Hz
6.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm300 kV/inASTM D149
Dissipation Factor  0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
ASTM D150
 0.11
@Frequency 60 Hz
0.11
@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 125 V125 VUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 171 °C340 °FASTM D648
UL RTI, Electrical 150 °C
@Thickness 1.57 mm
302 °F
@Thickness 0.0618 in
UL RTI, Mechanical with Impact 150 °C
@Thickness 1.57 mm
302 °F
@Thickness 0.0618 in
UL RTI, Mechanical without Impact 150 °C
@Thickness 1.57 mm
302 °F
@Thickness 0.0618 in
Flammability, UL94  V-0
@Thickness 3.18 mm
V-0
@Thickness 0.125 in
 V-0
@Thickness 3.18 mm
V-0
@Thickness 0.125 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
Quantum PEEK 30% Carbon Filled
Epoxy Technology EPO-TEK® T6067-T Thermally Conductive, Electrically Insulating Epoxy

PLEO918 / 50807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.