MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Spartech PP5930 Glass/Mica Reinforced Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Mica Filler

Material Notes:

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc
@Temperature 22.8 °C
1.14 g/cc
@Temperature 73.0 °F
ASTM D792
Filler Content 30 %30 %Glass/Mica
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/in0.125inch wall
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.4 MPa6000 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Elongation at Yield 2.0 %2.0 %ASTM D638
Flexural Modulus 3.79 GPa550 ksisecant; ASTM D790
 5.52 GPa800 ksitangent; ASTM D790
Izod Impact, Notched 0.534 J/cm
@Temperature 22.8 °C
1.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C260 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom TYC 727N C NATURAL Thermoplastic Olefinic Elastomer
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
LyondellBasell Petrothene NA594081 LDPE
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Compression Moldings

PSPAR120 / 78742

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.