MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Clearflex® MQ F0 Very Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Very Low Density Polyethylene (VLDPE)

Material Notes: Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).

The resin shows an excellent balance between flexibility and impact resistance.

Main Applications: Clearflex MQ F0 is suitable for injection molding. Products made with Clearflex MQ F0 are characterized by a high flexibility. Clearflex MQ F0 is recommended for seals and gaskets, for blend with polyolefins to modify and improve impact resistance.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.895 g/cc0.895 g/ccISO 1183
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 2626ISO 868/A
Tensile Strength at Break 9.00 MPa1310 psiISO 527
Tensile Strength, Yield 4.00 MPa580 psiISO 527
Elongation at Break 750 %750 %ISO 527
Flexural Modulus 0.0450 GPa6.53 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °FInternal method
Vicat Softening Point 51.0 °C
@Load 1.00 kg
124 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Orgalloy® LE 60 LM XV NAT Polyamide 6 Alloy
Celanese Zytel® ST811HS NC010 PA6-HI
Versalis Clearflex® MP D0 Very Low Density Polyethylene
Dow ATTANE™ 4206 Ultra Low Density Polyethylene, Impact Modifier Grade
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade

PENG085 / 124479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.