MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Orgalloy® LE 60 LM XV NAT Polyamide 6 Alloy
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Polyamide Alloy, Semi-Flexible grade, Nylon 6 based
Tubes / Mandrels / Profiles / Cables

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
 1.03 g/cc0.0372 lb/in³Cond.; ISO 1183
Water Absorption 5.5 %5.5 %Dry; Sim. to ISO 62
Moisture Absorption 1.50 %1.50 %Dry; Sim. to ISO 62
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 235 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 57
@Time 15.0 sec
57
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength, Yield 24.0 MPa3480 psiCond.; ISO 527-1/-2
 28.0 MPa4060 psiDry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 22 %22 %Dry; ISO 527-1/-2
 28 %28 %Cond.; ISO 527-1/-2
Tensile Modulus 0.650 GPa94.3 ksiCond.; ISO 527-1/-2
 0.850 GPa123 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  8.20 J/cm²
@Temperature 23.0 °C
39.0 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 8.90 J/cm²
@Temperature 23.0 °C
42.4 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 200 µm/m-°C111 µin/in-°FDry; ISO 11359-1/-2
Melting Point 220 °C428 °F10°C/min; Dry; ISO 11357-1/-3
Vicat Softening Point 86.0 °C187 °F50°C/h 50N; Dry; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
PlasticizerYes
Processing MethodsOther Extrusion
 Profile Extrusion
 Sheet Extrusion
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® ST811HS NC010 PA6-HI
Arkema Orgalloy® LE 6000 NAT Polyamide 6 Alloy
Versalis Clearflex® MP D0 Very Low Density Polyethylene
Versalis Clearflex® MQ F0 Very Low Density Polyethylene
Arkema Orgalloy® RS 6000 NAT Polyamide 6 Alloy

PARKG418 / 24494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.