System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Arkema Orgalloy® LE 60 LM XV NAT Polyamide 6 Alloy
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Unreinforced
Material Notes:
Polyamide Alloy, Semi-Flexible grade, Nylon 6 based
Tubes / Mandrels / Profiles / Cables
Information provided by Arkema Group
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.03
g/cc
ISO 1183
1.03
g/cc
Cond.; ISO 1183
Water Absorption
5.5 %
Dry; Sim. to ISO 62
Moisture Absorption
1.50 %
Dry; Sim. to ISO 62
Melt Flow
3.5
g/10 min
@Load 2.16 kg,
Temperature 235 °C
cm³/10 min Volumetric Rate; ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore D
57
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength, Yield
24.0
MPa
Cond.; ISO 527-1/-2
28.0
MPa
Dry; ISO 527-1/-2
Elongation at Break
>= 50 %
Dry; ISO 527-1/-2
>= 50 %
Cond.; ISO 527-1/-2
Elongation at Yield
22 %
Dry; ISO 527-1/-2
28 %
Cond.; ISO 527-1/-2
Tensile Modulus
650
MPa
Cond.; ISO 527-1/-2
850
MPa
Dry; ISO 527-1/-2
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched
82.0
kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
89.0
kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
Electrical Properties
Original Value
Comments
Comparative Tracking Index
600
V
Cond.; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
200
µm/m-°C
Dry; ISO 11359-1/-2
Melting Point
220
°C
10°C/min; Dry; ISO 11357-1/-3
Vicat Softening Point
86.0
°C
50°C/h 50N; Dry; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
IEC 60695-11-10
HB
@Thickness 3.20 mm
IEC 60695-11-10
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
Injection Molding; ISO 294
Mold Temperature
60.0
°C
Injection Molding; ISO 10724
Descriptive Properties
Form as Delivered
Pellets
Heat Stabilized
Yes
Light Stabilized
Yes
Moisture Sensitive
Yes
Plasticizer
Yes
Processing Methods
Other Extrusion
Profile Extrusion
Sheet Extrusion
Transfer Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Zytel® ST811HS NC010 PA6-HI
Arkema Orgalloy® LE 6000 NAT Polyamide 6 Alloy
Versalis Clearflex® MP D0 Very Low Density Polyethylene
Versalis Clearflex® MQ F0 Very Low Density Polyethylene
Arkema Orgalloy® RS 6000 NAT Polyamide 6 Alloy
PARKG418 / 24494
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.