MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Novatex® EP NLGI Grade 000
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Texaco Novatex EP are water resistant, extreme pressure greases. They are manufactured using highly refined, select high viscosity index base oils, a calcium soap, and a specifically selected additive package containing extreme pressure additives as well as corrosion and rust inhibitors.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 222318; MSDS Number: 9007

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 6262Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 1104 SUS1104 SUSSee Note 3.
Saybolt Viscosity at 210°F 80 SUS80 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 206 cSt206 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 15 cSt15 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 4646
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)
Four Ball Wear 0.400 mm0.0157 inScar Diameter
Penetration P(60), 1/10 mm 460460Unknown Amount of Work, 25°C (77°F)
Timken Test 18100 g40.0 lbOK Load
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FSee Note 2.
Minimum Service Temperature, Air -34.0 °C-29.2 °FSee Note 1.
Flash Point 162 °C324 °FSee Note 3.
 
Descriptive Properties
ColorRed-Brown
Corrosion, Copper Strip1B
TextureSemi-fluid
Thickener, %2Calcium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Marfak® 0
ChevronTexaco Novatex® EP NLGI Grade 1
ChevronTexaco Marfak® Heavy Duty 2
Phillips 66 EP Conolith® Grease NLGI NO. 000
ChevronTexaco Thuban® SAE 80W-90

WTEXA260 / 77139

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.