System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Kingfa UTPBT-HB Toughened PBT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Impact Grade
Material Notes:
Features:
High impact
Excellent size stability
Easy processing
Applications:
Injection molding
Switch parts
Keyboard keys
E & E parts
Information Provided by Kingfa Sci. & Tech. Co., Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.30
g/cc
@Temperature 23.0 °C
1.30
g/cc
@Temperature 73.4 °F
ASTM D792
Linear Mold Shrinkage
0.013
-
0.015
cm/cm
@Temperature 23.0 °C
0.013
-
0.015
in/in
@Temperature 73.4 °F
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
115
115
ASTM D785
Tensile Strength at Break
40.0
MPa
5800
psi
10mm/min; ASTM D638
Elongation at Break
60 %
60 %
10mm/min; ASTM D638
Flexural Strength
55.0
MPa
7980
psi
2mm/min; ASTM D790
Flexural Modulus
2.00
GPa
290
ksi
2mm/min; ASTM D790
Izod Impact, Notched
1.30
J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.44
ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
150
°C
@Thickness 6.40 mm
302
°F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
55.0
°C
@Thickness 6.40 mm
131
°F
@Thickness 0.252 in
ASTM D648
Flammability, UL94
HB
@Thickness 1.50 - 1.65 mm
HB
@Thickness 0.0591 - 0.0650 in
Processing Properties
Metric
English
Comments
Processing Temperature
<=
270
°C
<=
518
°F
Rear Barrel Temperature
220
-
240
°C
428
-
464
°F
Start Point: 230°C
Middle Barrel Temperature
235
-
255
°C
455
-
491
°F
Start Point: 245°C
Front Barrel Temperature
245
-
265
°C
473
-
509
°F
Start Point: 255°C
Melt Temperature
235
-
255
°C
455
-
491
°F
Start Point: 250°C
Mold Temperature
50.0
-
80.0
°C
122
-
176
°F
Start Point: 60°C
Drying Temperature
120
-
140
°C
@Time 14400 - 21600 sec
248
-
284
°F
@Time 4.00 - 6.00 hour
Pre-dry
Descriptive Properties
Injection Speed
Moderate to High
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
Kingfa PC-WT01 Weather Resistance PC
PKINGF001 / 104260
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.