MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 8103-13 One-Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested Uses: Casting; Potting; Encapsulating; Embedding applications where 2-component systems can not be used; Electronic and structural components, patterns, and medical equipment; Coating; Impregnation; Resurfacing; Insulation; Bonding metal, ceramics, glass, and most rigid materials; Assembly; Patching; and Filling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 600 cP600 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9898
Tensile Strength at Break 44.1 MPa6400 psi
Elongation at Break 3.3 %3.3 %
Flexural Strength 92.4 MPa13400 psi
Flexural Modulus 2.69 GPa390 ksi
Compressive Strength 90.3 MPa13100 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.62e+12 ohm-cm3.62e+12 ohm-cmC 96/23/96
 2.58e+15 ohm-cm2.58e+15 ohm-cm"A"
Surface Resistance 7.38e+11 ohm7.38e+11 ohmC 96/23/96
 2.36e+15 ohm2.36e+15 ohmCond. A
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
A
 3.27
@Frequency 60 Hz
3.27
@Frequency 60 Hz
A
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.167 - 0.201 W/m-K1.16 - 1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 104 °C219 °FDeflection Temp at unknown load
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 150 - 160 °C
1.00 - 2.00 hour
@Temperature 302 - 320 °F
 60.0 - 240 min
@Temperature 160 - 180 °C
1.00 - 4.00 hour
@Temperature 320 - 356 °F
optional
Pot Life 180 min
@Temperature 100 °C
180 min
@Temperature 212 °F
Shelf Life 5.00 - 8.00 Month5.00 - 8.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCast 8501-6 One-Component Epoxy
Abatron AboCast 10-5/AboCure 3-4 Epoxy
Abatron AboWeld 8708-5 One-Component Structural/Dielectric Epoxy
AGY ZenTron® S-2 Generic S-Glass Fiber
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled

PABC821 / 107805

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.