MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 5482 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for electrical insulating applications.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.660 g/cc0.0238 lb/in³ASTM D1895
Density 1.43 g/cc0.0517 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8888ASTM D785
Tensile Strength, Ultimate 64.0 MPa9280 psiASTM D638
Elongation at Break 0.92 %0.92 %ASTM D638
Tensile Modulus 8.70 GPa1260 ksiASTM D638
Flexural Strength 95.0 MPa13800 psiASTM D790
Flexural Modulus 7.40 GPa1070 ksiASTM D790
Compressive Strength 208 MPa30200 psiASTM D695
Izod Impact, Notched 0.163 J/cm0.305 ft-lb/inASTM D256
Charpy Impact, Notched 0.184 J/cm²0.876 ft-lb/in²ASTM D256
Impact 9999J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.60e+11 ohm-cm2.60e+11 ohm-cmASTM D247
Dielectric Constant 5.75.7ASTM D150
Dielectric Strength 9.10 kV/mm231 kV/inShort Time; ASTM D149
Dissipation Factor 0.0500.050ASTM D150
Arc Resistance 25 sec25 secASTM D495
Comparative Tracking Index 200 V200 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.0 µm/m-°C
@Temperature 40.0 - 130 °C
28.9 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.440 W/m-K
@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 200 °C392 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 157 °C315 °FASTM D648
Oxygen Index 28.3 %28.3 %ASTM D2863
Shrinkage 0.30 %0.30 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 5488 Phenolic, Granular, Injection Molded

PLEM03 / 50679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.