MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 5488 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not recommended for electrical insulating applications.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ASTM D1895
Density 1.45 g/cc0.0524 lb/in³ASTM D792
Water Absorption 0.267 %0.267 %ASTM D570
Linear Mold Shrinkage 0.0083 cm/cm0.0083 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8282ASTM D785
Tensile Strength, Ultimate 61.0 MPa8850 psiASTM D638
Elongation at Break 0.91 %0.91 %ASTM D638
Tensile Modulus 8.50 GPa1230 ksiASTM D638
Flexural Strength 93.0 MPa13500 psiASTM D790
Flexural Modulus 7.60 GPa1100 ksiASTM D790
Compressive Strength 189 MPa27400 psiASTM D695
Poissons Ratio 0.350.35ASTM D638
Shear Modulus 3.15 GPa457 ksiCalculated
Izod Impact, Notched 0.166 J/cm0.311 ft-lb/inASTM D256
Charpy Impact, Notched 0.178 J/cm²0.847 ft-lb/in²ASTM D256
Impact 100100J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+10 ohm-cm8.00e+10 ohm-cmASTM D247
Dielectric Constant 10.210.2ASTM D150
Dissipation Factor 0.0610.061ASTM D150
Arc Resistance 137 sec137 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.0 µm/m-°C
@Temperature 40.0 - 130 °C
25.6 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.510 W/m-K
@Temperature 100 °C
3.54 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 201 °C394 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 27.5 %27.5 %ASTM D2863
Shrinkage 0.269 %0.269 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 6401 Phenolic, Briquette, Injection Molded
Plenco 6343 Phenolic, Granular, Transfer Molded
Plenco 6301 Phenolic, Granular, Injection Molded
Plenco 6015 Phenolic, Briquette, Transfer Molded
Plenco 5350 Phenolic, Granular, Compression Molded

PLEM05 / 50681

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.