MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® HR92953 Medium Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: Applications
PETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black content of 2.6% and antioxidant has been added to ensure thermal stability during processing.

Processing Techniques
HR 92953, like other thermoplastic polyolefin compounds, can be extruded as wire and cable insulation using a conventional extruder. Below are suggested extrusion conditions for HR 92953. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size, affect the processing of thermoplastic compounds.

This product is from the former Equistar product line.

Key Words: MDPE; Telecom/ Telecommunications; Jacketing; Black Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D1505
ESCR 10% Igepal® >= 1000 hour>= 1000 hourASTM D1693
Absorption Coefficient 450450ASTM D3349
Carbon Black Loading 2.6 %2.6 %
Melt Flow 0.65 g/10 min0.65 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength at Break 27.6 MPa4000 psiASTM D638
Tensile Strength, Yield 16.5 MPa2400 psiASTM D638
Elongation at Break 880 %880 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.55
@Frequency 1e+6 Hz
2.55
@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 21.7 kV/mm550 kV/inDC; ASTM D149
Dissipation Factor 0.00050
@Frequency 1e+6 Hz
0.00050
@Frequency 1e+6 Hz
ASTM D1531
 
Thermal PropertiesMetricEnglishComments
CTE, linear 175 µm/m-°C
@Temperature 20.0 °C
97.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Processing PropertiesMetricEnglishComments
Feed Temperature 154 - 163 °C310 - 325 °F
Zone 2 177 - 193 °C350 - 380 °F
Zone 3 193 - 210 °C380 - 410 °F
Zone 4-x 204 - 218 °C400 - 425 °F
Adapter Temperature 204 - 218 °C400 - 425 °F
Die Temperature 204 - 218 °C400 - 425 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene
LyondellBasell Petrothene® GA837091 Linear Medium Density Polyethylene
LyondellBasell Petrothene® KR92717 High Density Polyethylene
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene
Total HP 401 MDPE, pipe, cable, sheet

PEQU0252 / 36686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.