MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC FL1680 Lubricant Powder
Categories: Fluid; Lubricant

Material Notes: Description: FL1680 lubricant is a white, finely divided, low molecular weight powder manufactured from virgin PTFE feedstock. It has an average particle size of 11 microns, a narrow particle size distribution and low surface area. FL1680 is virtually immune from chemical attack, is water repellent, has good electrical insulation properties, a wide working temperature range and has excellent weathering and ageing characteristics.

Applications: FL1680 is primarily used as an additive in other materials to improve wear resistance and enhance lubricity, non-stick and frictional characteristics of the host media. It may be incorporated into products such as printing inks, oils, greases and industrial finishes. FL1680 is particularly suitable for use in printing inks and industrial finishes due to its fine particle size but may also be used in oil, grease and sealing paste applications where low starting torque and a smooth sliding action is required. Lubricant powder applications, properties and processing data are contained in the Lubricant Applications Brochure, available upon request.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.20 g/cc2.20 g/cc
Bulk Density 0.450 g/cc0.0163 lb/in³
Particle Size 5.0 µm5.0 µmD10
 9.0 µm9.0 µmHegmann gauge
 11 µm11 µmOptical Microscope
 15 µm15 µmD50
 35 µm35 µmD90
Specific Surface Area 0.80 m²/g0.80 m²/gKrypton
 
Thermal PropertiesMetricEnglishComments
Melting Point 328 °C622 °FD.S.C.
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -190 °C-310 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Dow UCON™ 50-HB-660 Fluids and Lubricants
ChevronTexaco Delo® 400 SAE 20

PAGCX121 / 191230

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.