MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 2061-15 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-15 provides excellent heat resistance, impact strength, and processability. CALIBRE 2061-6 resin is compliant with ISO 10993 (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications. This product contains mold release and is currently available in black color.

Main Characteristics:

  • ISO 10993
Applications:
  • Medical applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/A
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
0.32 %
@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
15 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7373ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 68.0 MPa9860 psiISO 527-2/50
 68.3 MPa9910 psi50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa8990 psiISO 527-2/50
 62.1 MPa9010 psi50 mm/min; ASTM D638
Elongation at Break 150 %150 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638; ISO 527-2/50
Tensile Modulus 2.21 GPa321 ksi50 mm/min; ASTM D638
 2.30 GPa334 ksiISO 527-2/50
Flexural Strength 96.5 MPa14000 psiMethod I (3 point load), 2.0 mm/min; ASTM D790
 98.0 MPa14200 psi2.0 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2.0 mm/min; ISO 178
 2.41 GPa350 ksiMethod I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 7.50 J/cm
@Temperature 23.0 °C
14.1 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 74.0 kJ/m²
@Temperature 23.0 °C
35.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Impact Strength 378 kJ/m²180 ft-lb/in²ASTM D1822
Dart Drop, Total Energy 81.3 J60.0 ft-lb3.39 m/sec; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmASTM D257
Dielectric Constant  3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
 17.0 kV/mm432 kV/inIEC 60243-1
Dissipation Factor  0.0010
@Frequency 50 Hz
0.0010
@Frequency 50 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 180 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 139 °C282 °FAnnealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FUnannealed; ISO 75-2/A
 122 °C252 °FUnannealed; ASTM D648
 136 °C277 °FAnnealed; ASTM D648; ISO 75-2/A
Vicat Softening Point 143 °C289 °FISO 306/B50
 148 °C
@Load 5.10 kg
298 °F
@Load 11.2 lb
Rate A (50°C/h); ASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542; ISO 489
Haze 1.0 %1.0 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 2061-22 Polycarbonate Resin
Overview of materials for Polycarbonate, Optical Grade
Dow Tyril® 100 SAN
Trinseo CALIBRE™ 5101-15 Polycarbonate Resin
Trinseo CALIBRE™ 5201-8 Polycarbonate Resin

PZZDWST027 / 142236

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.