MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toray TOYOLAC™ ABS Resin VX10-X01 ABS/PBT Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: ABS/PBT Alloy, PBT+ABS.

General Toyolac™ Notes: TOYOLAC™ ABS is a versatile thermoplastic consisting of acrylonitrile, butadiene, and styrene and it has unique set of properties combining strength, lightness, and aesthetics. TOYOLAC™ is widely used in both industrial and household goods due to its excellent mechanical, chemical, electrical properties, and superior processability.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm0.0060 - 0.0090 in/in23°C/50% RH; Toray Method
Melt Flow 21 g/10 min
@Load 9.99 kg,
Temperature 240 °C
21 g/10 min
@Load 22.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R  108
@Temperature 23.0 °C
108
@Temperature 73.4 °F
50% RH; ASTM D785
 108
@Temperature 23.0 °C
108
@Temperature 73.4 °F
ISO 2039-2
Tensile Strength 43.0 MPa6240 psiASTM D638
 45.0 MPa
@Temperature 23.0 °C
6530 psi
@Temperature 73.4 °F
ISO 527-1,2
Elongation at Break 50 %50 %ASTM D638
 10 %
@Temperature 23.0 °C
10 %
@Temperature 73.4 °F
ISO 527-1,2
Flexural Strength 66.0 MPa9570 psiASTM D790
 68.0 MPa
@Temperature 23.0 °C
9860 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 1.93 GPa280 ksiASTM D790
 1.98 GPa
@Temperature 23.0 °C
287 ksi
@Temperature 73.4 °F
50% RH; ISO 178
Izod Impact, Notched  0.690 J/cm
@Thickness 12.7 mm,
Temperature -30.0 °C
1.29 ft-lb/in
@Thickness 0.500 in,
Temperature -22.0 °F
V-notched; ASTM D256
 1.02 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
1.91 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
V-notched; ASTM D256
 2.00 J/cm
@Thickness 12.7 mm,
Temperature 23.0 °C
3.75 ft-lb/in
@Thickness 0.500 in,
Temperature 73.4 °F
V-notched; ASTM D256
 4.70 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
8.81 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
V-notched; ASTM D256
Charpy Impact, Notched 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
V-Notched; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FISO 75-1,2
 92.0 °C198 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9244 / 248933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.