MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Starflam® PW0042E PA6-MF20 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Mineral Filled

Material Notes: Starflam PW0042E is a mineral filled, flame retardant PA6 for injection molded applications. The material is halogen free and red phosphorus free.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³DAM; ISO 1183
Water Absorption 1.4 %
@Temperature 23.0 °C,
Time 86400 sec
1.4 %
@Temperature 73.4 °F,
Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.7 %
@Temperature 23.0 °C
1.7 %
@Temperature 73.4 °F
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cm
@Thickness 2.00 mm
0.011 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
0.010 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 33.0 MPa4790 psi50% RH; ISO 527-2
 73.0 MPa10600 psiDAM; ISO 527-2
Elongation at Break 2.8 %2.8 %DAM; ISO 527-2
 12 %12 %50% RH; ISO 527-2
Tensile Modulus 2.20 GPa319 ksi50% RH; ISO 527-2
 5.20 GPa754 ksiDAM; ISO 527-2
Flexural Strength 40.0 MPa5800 psi50% RH; ISO 178
 109 MPa15800 psiDAM; ISO 178
Flexural Modulus 2.10 GPa305 ksi50% RH; ISO 178
 5.20 GPa754 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  2.70 kJ/m²
@Temperature -30.0 °C
1.28 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 2.70 kJ/m²
@Temperature -40.0 °C
1.28 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 3.10 kJ/m²
@Temperature -40.0 °C
1.48 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 3.40 kJ/m²
@Temperature -30.0 °C
1.62 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 3.90 kJ/m²
@Temperature 23.0 °C
1.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 4.90 kJ/m²
@Temperature 23.0 °C
2.33 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
Charpy Impact Unnotched  3.00 J/cm²
@Temperature -40.0 °C
14.3 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 3.10 J/cm²
@Temperature -30.0 °C
14.8 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 3.10 J/cm²
@Temperature -40.0 °C
14.8 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eU
 3.60 J/cm²
@Temperature -30.0 °C
17.1 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 3.80 J/cm²
@Temperature 23.0 °C
18.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 7.60 J/cm²
@Temperature 23.0 °C
36.2 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  0.210 J/cm²
@Temperature -40.0 °C
0.999 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.220 J/cm²
@Temperature -30.0 °C
1.05 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.260 J/cm²
@Temperature -30.0 °C
1.24 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.260 J/cm²
@Temperature -40.0 °C
1.24 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.310 J/cm²
@Temperature 23.0 °C
1.48 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.410 J/cm²
@Temperature 23.0 °C
1.95 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  21.0 kV/mm
@Thickness 1.00 mm
533 kV/in
@Thickness 0.0394 in
50% RH; IEC 60243
 25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 188 °C370 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
Flammability, UL94 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature >= 240 °C>= 464 °FInjection
 <= 250 °C<= 482 °FInjection
Middle Barrel Temperature >= 250 °C>= 482 °FInjection
 <= 260 °C<= 500 °FInjection
Front Barrel Temperature >= 250 °C>= 482 °FInjection
 <= 270 °C<= 518 °FInjection
Melt Temperature >= 250 °C>= 482 °FInjection
 <= 270 °C<= 518 °FInjection
Mold Temperature >= 50.0 °C>= 122 °FInjection
 <= 90.0 °C<= 194 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesFlame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9123 / 287574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.