System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
38
materials in the category
Nylon 6, 20% Mineral Filled
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
38
Results
-- Page
1
of
1
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for Nylon 6, 20% Mineral Filled
2
Mocom (ALBIS) ALTECH® PA6 A 4012/500 MR12 Nylon 6, 12% Mineral Fiber Reinforced
3
Mocom (ALBIS) ALTECH® PA6 A 4012/500 MR12 WT 1137-13 Nylon 6, 12% Mineral Fiber Reinforced
4
Mocom (ALBIS) ALTECH® PA6 A 4012/520 MR12 WT 1137-13 Nylon 6, 12% Mineral Fiber Reinforced
5
Mocom (ALBIS) ALTECH® PA6 A 4020/100 MR20 Nylon 6, 20% Mineral Fiber Reinforced
6
ALM Ultrasint® PA6 MF Nylon 6, Mineral Reinforced, Dry
7
ALM Ultrasint® PA6 MF Nylon 6, Mineral Reinforced, Conditioned
8
Ascend Performance Materials Starflam® PW0042E PA6-MF20 FR
9
Eurotec® Tecomid® NB40 MF20 GR003 FY70 PA6, 20% mineral filled, flame retardant - halogen free (RoHS compliant), grey RAL 7035
10
Ascend Performance Materials Starflam® PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
11
GLS Polymers PW39 Nylon 6, 15% Mineral Reinforced, Precolor
12
Zhejiang Juner PA-A6-1 MF25%
13
LATI KELON B FR H CET/05-V2 5% Mineral Filled, Heat-Stabilized Nylon 6
14
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose
15
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose
16
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact
17
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact
18
Cheng Yu Plastic N6C1 Nylon 6, 10% Mineral Reinforced
19
Cheng Yu Plastic N6C2 Nylon 6, 20% Mineral Reinforced
20
Cheng Yu Plastic N6CV1 Flame Retardant Nylon 6, 10% Mineral Reinforced
21
Cheng Yu Plastic NGCV2 Flame Retardant Nylon 6, 20% Mineral Reinforced
22
Omni Plastics OmniLon™ 6 PA6 WF20 Mineral Filled Nylon
23
Petropol Nypol® B3 T10 TZ PRTA011 NT382 Nylon 6, 10% Mineral Reinforced
24
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc
25
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling
26
Polyplastic Compounds Armamid® PA6 GF 20-5FRM Nylon 6, 20% Mineral Fiber Reinforced
27
Polyplastic Compounds Armamid® PA6 MiF 20-1FR Nylon 6, 20% Mineral Fiber Reinforced
28
Polyplastic Compounds Armamid® PA6 MF 15-1 Nylon 6, 15% Mineral Fiber Reinforced
29
Polyplastic Compounds Armamid® PA6 MF 15-2 Nylon 6, 15% Mineral Fiber Reinforced
30
Polyram PlusTek PB350M4 Nylon 6, 20% Mineral Filled
31
RTP Company RTP 225 A Nylon 6 (PA), Mineral
32
Ravago Manufacturing Americas Hylon N2020MHL Nylon 6, 20% Mineral Filled, DAM
33
Ravago Manufacturing Americas Enviramid N2320MHL BK Nylon 6, 20% Mineral Filled, DAM
34
Teknor Apex Chemlon® MDM54 Nylon 6, Dry, Mineral Reinforced
35
Teknor Apex Chemlon® MDM54 Nylon 6, Conditioned, Mineral Reinforced
36
Toyobo GLAMIDE® T-422VOR Nylon-6
37
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry
38
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Conditioned
Found
38
Results
-- Page
1
of
1
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.