LATI Latistat 52/7-02 MI/30 PP Homopolymer, 30% Mica Filled
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 30% Mica Filler
Material Notes:
Dissipative product based on Polypropylene homopolymer (PPh). Mica filler.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.22
g/cc
0.0441
lb/in³
Linear Mold Shrinkage, Flow
0.0080
-
0.010
cm/cm
0.0080
-
0.010
in/in
Linear Mold Shrinkage, Transverse
0.0085
-
0.0105
cm/cm
0.0085
-
0.0105
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
30.0
MPa
4350
psi
Elongation at Break
3.0 %
3.0 %
Elongation at Yield
1.5 %
1.5 %
Tensile Modulus
5.20
GPa
754
ksi
Charpy Impact Unnotched
1.00
J/cm²
4.76
ft-lb/in²
Charpy Impact, Notched
0.100
J/cm²
0.476
ft-lb/in²
Electrical Properties
Metric
English
Comments
Surface Resistance
800
ohm
800
ohm
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
140
°C
284
°F
Deflection Temperature at 1.8 MPa (264 psi)
95.0
°C
203
°F
Vicat Softening Point
110
°C
@Load 5.00 kg
230
°F
@Load 11.0 lb
Processing Properties
Metric
English
Comments
Melt Temperature
200
-
240
°C
392
-
464
°F
Mold Temperature
40.0
-
60.0
°C
104
-
140
°F
Drying Temperature
80.0
-
90.0
°C
@Time 10800 sec
176
-
194
°F
@Time 3.00 hour
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436M30L Mica Reinforced
Aclo Accutech Polypropylene Copolymer CP0437M30L Mica Reinforced
Lushan PP+GF30% Maleic Anhydride Grafted Polypropylene
Crystex Composites Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced
PLATH9980 / 177676
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.