MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Udel® GF-110 PSU, 10% glass fiber
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 10% Glass Fiber Reinforced

Material Notes: Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the polysulfone resin. The high performance properties and attractive price make these resins particularly effective alternatives to metals in many engineering applications.

- Natural: Udel® GF-110 NT

Applications: Appliance Components; Appliances; Connectors; Fittings; Food Service Applications; Industrial Parts; Microwave Cookware; Plumbing Parts; Valves/Valve Parts

Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Strength; High Heat Resistance; High Rigidity; Hydrocarbon Resistant; Hydrolytically Stable

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inASTM D955
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 343 °C
6.5 g/10 min
@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 77.9 MPa11300 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Tensile Modulus 3.72 GPa540 ksiASTM D638
Flexural Strength 128 MPa18600 psiASTM D790
Flexural Modulus 3.79 GPa550 ksiASTM D790
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
Tensile Impact Strength 101 kJ/m²48.1 ft-lb/in²ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+16 ohm-cm3.00e+16 ohm-cmASTM D257
Dielectric Constant  3.15
@Frequency 1e+6 Hz
3.15
@Frequency 1e+6 Hz
ASTM D150
 3.18
@Frequency 60 Hz
3.18
@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm483 kV/inASTM D149
Dissipation Factor  0.00070
@Frequency 60 Hz
0.00070
@Frequency 60 Hz
ASTM D150
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 179 °C354 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 343 - 399 °C649 - 750 °FInjection
Mold Temperature 121 - 163 °C250 - 325 °F
Drying Temperature 149 - 163 °C300 - 325 °F
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color; Opaque
FormsPellets
Injection RateFast
ProcessingExtrusion; Injection Molding
RoHS ComplianceYes
Screw Compression Ratio2.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4575 / 280375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.