MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese ZENITE ZE55201 LCP, 50% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Material Notes: Zenite« ZE55201 is a 50% mineral/glass fiber reinforced liquid crystal polymer for injection molding. and It is specifically suitable for applications requiring ultra flatness.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³ISO 1183
Density of Compound 1.62 g/cc0.0585 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 88.0 MPa12800 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.4 %1.4 %5mm/min; ISO 527-2/1A
Tensile Modulus 15.8 GPa2290 ksi50mm/min; ISO 527-2/1A
Flexural Strength 165 MPa23900 psiISO 178
Flexural Modulus 12.5 GPa1810 ksiISO 178
Compressive Strength 21.3 MPa
@Strain 1 %
3090 psi
@Strain 1 %
ISO 604
Charpy Impact, Notched 0.360 J/cm²1.71 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 37.0 kV/mm940 kV/inIEC 60243-1
Dissipation Factor  0.031
@Frequency 1e+6 Hz
0.031
@Frequency 1e+6 Hz
IEC 60250
 0.031
@Frequency 100 Hz
0.031
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 27.0 µm/m-°C15.0 µin/in-°FISO 11359-2
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Melting Point 335 °C635 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 300 °C572 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FISO 75-1, -2
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Oxygen Index 41 %41 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
Feed Temperature 40.0 - 60.0 °C104 - 140 °F
Zone 1 320 - 330 °C608 - 626 °F
Zone 2 335 - 345 °C635 - 653 °F
Zone 3 335 - 345 °C635 - 653 °F
Zone 4 335 - 345 °C635 - 653 °F
Die Temperature 335 - 345 °C635 - 653 °F
Melt Temperature 330 - 350 °C626 - 662 °F
Ejection Temperature 270 °C518 °F
Drying Temperature >= 150 °C>= 302 °F
Dry Time 3.00 hour3.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 50.0 - 150 MPa7250 - 21800 psi
Back Pressure <= 3.00 MPa<= 435 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zenite® 6130 WT010 30% GF LCP (Extended Tabular Temperature Data)
Celanese ZENITE 5130L LCP, 30% Glass Reinforced
Celanese Zenite® 7130 WT010 LCP (Extended Tabular Temperature Data)
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese Zenite® 6130LX WT010 LCP

PHCQ546 / 179001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.