MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® Care ML-GB30 Nylon 12, 30% Glass Bead Filled, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Glass Bead Filled

Material Notes: Microglass bead-filled (30%) PA12 resin for the injection molding of rigid, low-warpage and dimensionally accurate moldings
Industrial Sector: Sustainable, Industry and Engineering, Medical Devices
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Conformity: Biocompatibility, Medical application
Additives: Glass beads / spheres
Applications: Encapsulation
Regulatory: US Pharmacopeia Class VI conformity

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Water Absorption 0.0110 %0.0110 %Sim to ISO 62
Moisture Absorption 0.00500 %0.00500 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00600 cm/cm0.00600 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00700 cm/cm0.00700 in/inISO 294-4, 2577
Melt Flow 100 g/10 min
@Load 5.00 kg,
Temperature 275 °C
100 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 37.0 MPa5370 psiISO 527
Tensile Strength 47.0 MPa6820 psiISO 527
Tensile Strength, Yield 47.0 MPa6820 psiISO 527
Elongation at Break 20.0 %20.0 %Nominal; ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 2.10 GPa305 ksiISO 527
Charpy Impact Unnotched  16.0 J/cm²
@Temperature 23.0 °C
76.1 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eU
 16.0 J/cm²
@Temperature -30.0 °C
76.1 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched  0.440 J/cm²
@Temperature 23.0 °C
2.09 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cm?V; IEC 62631-3-1
Dielectric Constant  3.50
@Frequency 1.00e+6 Hz
3.50
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 4.10
@Frequency 100 Hz
4.10
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 36.0 kV/mm
@Thickness 1.00 mm
914 kV/in
@Thickness 0.0394 in
AC, S20/S20, t.; IEC 60243-1
Dissipation Factor  0.0230
@Frequency 1.00e+6 Hz
0.0230
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0310
@Frequency 100 Hz
0.0310
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  130 µm/m-°C
@Temperature 25.0 - 55.0 °C
72.2 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
 130 µm/m-°C
@Temperature 25.0 - 55.0 °C
72.2 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75-1/-2
Vicat Softening Point 155 °C
@Load 5.10 kg
311 °F
@Load 11.2 lb
50 K/h; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FInjection Molding; ISO 294
 250 °C482 °F
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
 80.0 °C176 °F
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Hold Pressure 70.0 MPa10200 psiInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption23.9 kgISO 14040, 14044
Global Warming Potential2.4 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 4.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 4.9 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7878 / 325010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.