MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes: Ensinger’s DELRIN®100AF blend stock shapes are a 13% PTFE fiber filled homopolymer acetal. They offer an improved coefficient of friction, better lubricity, and improved wear characteristics over unfilled and PTFE powder filled acetals. This advanced acetal material uses a combination of PTFE fibers uniformly dispersed in Delrin acetal resin. The combination results in improved wear characteristics along with strength, toughness, dimensional stability and machinability. The materials exceptional wear properties and internal lubrication serves to reduce or eliminate the need for external lubricants. Ensinger can also produce a full strength 20% PTFE filled version.
  • Excellent wear characteristics
  • Self lubricating
  • Low coefficient of friction
  • Maximum unmodified toughness
  • Superior load bearing characteristics
DELRIN®100AF is often used for applications such as bearing, bushings, cams and other antifriction devices that also require extra toughness.

Information provided by Ensinger

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D792
Density 1.49 g/cc0.0540 lb/in³ASTM D792
Water Absorption 0.12 %
@Time 86400 sec
0.12 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7777ASTM D785
Tensile Strength, Yield 54.25 MPa7868 psiASTM D638
Elongation at Yield 10.3 %10.3 %ASTM D638
Tensile Modulus 2.36 GPa342 ksi1mm/min; ASTM D638
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 175 °C347 °FASTM D3418
Maximum Service Temperature, Air 85.0 °C185 °Flong term
 149 °C300 °Fintermittent
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM)
Delrin Delrin® 100AF POM-PTFE20
Ensinger Delrin® 150 Homopolymer Acetal (POM)
Delrin Delrin® 100 NC010 POM
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM)

PENSIN096 / 122206

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.