MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® CD 2005 Polycarbonate, Optical/Compact Disc Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Injection molding grade with exceptionally good flow, for optical storage media such as CD.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Moisture Absorption at Equilibrium 0.15 %0.15 %50% RH
Water Absorption at Saturation 0.35 %0.35 %
 0.35 %0.35 %
Melt Flow 60 g/10 min
@Load 1.20 kg,
Temperature 300 °C
60 g/10 min
@Load 2.65 lb,
Temperature 572 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi
Elongation at Break >= 50 %>= 50 %Nominal
Elongation at Yield 6.0 %6.0 %
Tensile Modulus 2.30 GPa334 ksi
Charpy Impact Unnotched NBNB
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
Dielectric Strength 30.0 kV/mm762 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 137 °C279 °F
Deflection Temperature at 1.8 MPa (264 psi) 122 °C252 °F
Vicat Softening Point 143 °C289 °F
Glass Transition Temp, Tg 145 °C293 °F
UL RTI, Electrical 75.0 °C
@Thickness 0.710 mm
167 °F
@Thickness 0.0280 in
UL RTI, Mechanical with Impact 75.0 °C
@Thickness 0.710 mm
167 °F
@Thickness 0.0280 in
UL RTI, Mechanical without Impact 75.0 °C
@Thickness 0.710 mm
167 °F
@Thickness 0.0280 in
Flammability, UL94 V-2
@Thickness 0.710 mm
V-2
@Thickness 0.0280 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5831.583DIN 5026-1
Transmission, Visible >= 89 %
@Thickness 1.00 mm
>= 89 %
@Thickness 0.0394 in
ISO 489-A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 305 - 335 °C581 - 635 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyimide
Celanese Celstran® PA66-GF30-02 Nylon 66, 30% Glass Reinforced
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized
Envalior Akulon® SG-KGS6 PA66-GF30 FR
Teijin Panlite® AD-5503 Optical Use Polycarbonate Resin

PBA459 / 26960

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.