MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.00545 - 1.95 g/cc0.000197 - 0.0704 lb/in³Average value: 1.38 g/cc Grade Count:200
Filler Content 0.000 - 40.0 %0.000 - 40.0 %Average value: 22.9 % Grade Count:33
Water Absorption 0.0400 - 2.00 %0.0400 - 2.00 %Average value: 0.530 % Grade Count:99
 0.260 - 3.15 %
@Temperature 50.0 - 80.0 °C
0.260 - 3.15 %
@Temperature 122 - 176 °F
Average value: 1.60 % Grade Count:17
 0.300 - 3.29 %
@Temperature 50.0 - 80.0 °C
0.300 - 3.29 %
@Temperature 122 - 176 °F
Average value: 1.60 % Grade Count:14
 0.300 - 3.29 %
@Time 86400 - 173000 sec
0.300 - 3.29 %
@Time 24.0 - 48.0 hour
Average value: 1.60 % Grade Count:14
Moisture Absorption at Equilibrium 0.0200 - 3.90 %0.0200 - 3.90 %Average value: 0.480 % Grade Count:43
Water Absorption at Saturation 0.420 - 4.00 %0.420 - 4.00 %Average value: 1.78 % Grade Count:33
 2.30 - 4.17 %
@Temperature 80.0 - 80.0 °C
2.30 - 4.17 %
@Temperature 176 - 176 °F
Average value: 3.20 % Grade Count:3
Viscosity  8.00 - 16.0 cP
@Temperature 360 - 360 °C
8.00 - 16.0 cP
@Temperature 680 - 680 °F
Average value: 9.60 cP Grade Count:15
 8.00 - 16.0 cP
@Load 5.00 - 5.00 kg
8.00 - 16.0 cP
@Load 11.0 - 11.0 lb
Average value: 9.60 cP Grade Count:15
Thickness 5.00 - 127 microns0.197 - 5.00 milAverage value: 72.2 microns Grade Count:3
Linear Mold Shrinkage 0.000100 - 0.0140 cm/cm0.000100 - 0.0140 in/inAverage value: 0.00634 cm/cm Grade Count:45
Linear Mold Shrinkage, Transverse 0.00500 - 0.0140 cm/cm0.00500 - 0.0140 in/inAverage value: 0.00671 cm/cm Grade Count:14
Melt Flow 2.00 - 37.0 g/10 min2.00 - 37.0 g/10 minAverage value: 15.2 g/10 min Grade Count:22
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 20.0 - 91.020.0 - 91.0Average value: 55.6 Grade Count:11
Hardness, Rockwell M 20.0 - 12520.0 - 125Average value: 103 Grade Count:26
Hardness, Rockwell R 74.0 - 12974.0 - 129Average value: 117 Grade Count:6
Hardness, Shore D 65.0 - 93.065.0 - 93.0Average value: 85.4 Grade Count:60
Ball Indentation Hardness 138 - 345 MPa20000 - 50000 psiAverage value: 163 MPa Grade Count:14
Tensile Strength, Ultimate 0.0480 - 345 MPa6.96 - 50000 psiAverage value: 95.1 MPa Grade Count:164
 23.0 - 324.054 MPa
@Temperature 150 - 260 °C
3340 - 47000.1 psi
@Temperature 302 - 500 °F
Average value: 86.1 MPa Grade Count:34
Tensile Strength, Yield 15.0 - 230 MPa2180 - 33300 psiAverage value: 103 MPa Grade Count:44
 27.579 - 141.343 MPa
@Temperature 149 - 260 °C
4000.0 - 20500.0 psi
@Temperature 300 - 500 °F
Average value: 88.8 MPa Grade Count:6
Elongation at Break 0.350 - 200 %0.350 - 200 %Average value: 15.7 % Grade Count:164
 1.70 - 90.0 %
@Temperature 150 - 260 °C
1.70 - 90.0 %
@Temperature 302 - 500 °F
Average value: 11.3 % Grade Count:26
Elongation at Yield 2.00 - 90.0 %2.00 - 90.0 %Average value: 8.77 % Grade Count:23
 4.00 - 90.0 %
@Temperature 149 - 149 °C
4.00 - 90.0 %
@Temperature 300 - 300 °F
Average value: 25.5 % Grade Count:4
Modulus of Elasticity 0.107 - 46.9 GPa15.5 - 6800 ksiAverage value: 5.92 GPa Grade Count:119
 1.03421 - 3.71627 GPa
@Temperature 260 - 260 °C
150.002 - 539.008 ksi
@Temperature 500 - 500 °F
Average value: 2.29 GPa Grade Count:7
Flexural Yield Strength 24.8 - 490 MPa3600 - 71000 psiAverage value: 151 MPa Grade Count:164
 20.6843 - 344.738 MPa
@Temperature 149 - 260 °C
3000.01 - 50000.1 psi
@Temperature 300 - 500 °F
Average value: 128 MPa Grade Count:31
Flexural Modulus 1.38 - 40.0 GPa200 - 5800 ksiAverage value: 6.47 GPa Grade Count:147
 0.0102 - 30.3 GPa
@Temperature 149 - 300 °C
1.48 - 4390 ksi
@Temperature 300 - 572 °F
Average value: 7.80 GPa Grade Count:30
Flexural Strain at Break 1.30 - 5.50 %1.30 - 5.50 %Average value: 3.34 % Grade Count:13
Flexural Strain at Yield 1.40 - 7.90 %1.40 - 7.90 %Average value: 4.08 % Grade Count:27
Compressive Strain at Break 12.0 - 54.0 %12.0 - 54.0 %Average value: 27.1 % Grade Count:12
 21.0 - 31.0 %
@Temperature 260 - 260 °C
21.0 - 31.0 %
@Temperature 500 - 500 °F
Average value: 26.3 % Grade Count:2
Compressive Yield Strength 0.00217 - 570 MPa0.315 - 82700 psiAverage value: 164 MPa Grade Count:99
 71.0 - 414 MPa
@Temperature 149 - 260 °C
10300 - 60000 psi
@Temperature 300 - 500 °F
Average value: 136 MPa Grade Count:9
 96.0 - 172 MPa
@Temperature 260 - 260 °C
13900 - 24900 psi
@Temperature 500 - 500 °F
Average value: 136 MPa Grade Count:2
 96.0 - 172 MPa
@Strain 10.0 - 10.0 %
13900 - 24900 psi
@Strain 10.0 - 10.0 %
Average value: 136 MPa Grade Count:2
Compressive Modulus 0.00164 - 7.94 GPa0.238 - 1150 ksiAverage value: 2.85 GPa Grade Count:53
 1.663 - 2.997 GPa
@Temperature 260 - 260 °C
241.2 - 434.7 ksi
@Temperature 500 - 500 °F
Average value: 2.17 GPa Grade Count:3
Poissons Ratio 0.250 - 0.4100.250 - 0.410Average value: 0.370 Grade Count:4
 0.320 - 0.320
@Temperature 190 - 190 °C
0.320 - 0.320
@Temperature 374 - 374 °F
Average value: 0.320 Grade Count:1
Fatigue Strength  16.5474 - 26.2001 MPa
@# of Cycles 1000 - 1.00e+7
2400.00 - 3800.01 psi
@# of Cycles 1000 - 1.00e+7
Average value: 21.4 MPa Grade Count:1
 16.5474 - 26.2001 MPa
@Temperature 260 - 260 °C
2400.00 - 3800.01 psi
@Temperature 500 - 500 °F
Average value: 21.4 MPa Grade Count:1
Shear Strength 81.4 - 90.0 MPa11800 - 13100 psiAverage value: 87.8 MPa Grade Count:4
 78.5 - 78.5 MPa
@Temperature 150 - 150 °C
11400 - 11400 psi
@Temperature 302 - 302 °F
Average value: 78.5 MPa Grade Count:1
Izod Impact 25.0 - 69.0 J18.4 - 50.9 ft-lbAverage value: 56.2 J Grade Count:19
 38.0 - 74.0 J
@Temperature -30.0 - -30.0 °C
28.0 - 54.6 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 66.8 J Grade Count:15
Izod Impact, Notched 0.0700 - 9.20 J/cm0.131 - 17.2 ft-lb/inAverage value: 1.05 J/cm Grade Count:65
Izod Impact, Unnotched 0.900 - 5340 J/cm1.69 - 10000 ft-lb/inAverage value: 8.26 J/cm Grade Count:41
Izod Impact, Notched (ISO) 0.0430 - 27.0 kJ/m²0.0205 - 12.8 ft-lb/in²Average value: 5.71 kJ/m² Grade Count:23
 4.00 - 5.00 kJ/m²
@Temperature -30.0 - -30.0 °C
1.90 - 2.38 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.80 kJ/m² Grade Count:15
Izod Impact, Unnotched (ISO) 0.320 kJ/m² - NB0.152 ft-lb/in² - NBAverage value: 87.6 kJ/m² Grade Count:18
 147 kJ/m² - NB
@Temperature -30.0 - -30.0 °C
69.9 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 147 kJ/m² Grade Count:15
Charpy Impact Unnotched 0.540 J/cm² - NB2.57 ft-lb/in² - NBAverage value: 3.62 J/cm² Grade Count:52
 999.9 - 999.9 J/cm²
@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Grade Count:12
Charpy Impact, Notched 0.110 - 1.60 J/cm²0.524 - 7.61 ft-lb/in²Average value: 0.423 J/cm² Grade Count:49
Dart Drop, Total Energy 33.0 J24.3 ft-lbAverage value: 33.0 J Grade Count:15
Coefficient of Friction 0.0600 - 0.4900.0600 - 0.490Average value: 0.237 Grade Count:18
Coefficient of Friction, Static 0.200 - 0.3500.200 - 0.350Average value: 0.294 Grade Count:5
K Factor (Wear Factor) 0.400 - 13.10.400 - 13.1Average value: 5.48 Grade Count:3
Compression Set 12.5 - 98.0 %12.5 - 98.0 %Average value: 45.3 % Grade Count:26
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.100 - 4.00e+19 ohm-cm0.100 - 4.00e+19 ohm-cmAverage value: 9.34e+17 ohm-cm Grade Count:51
Surface Resistance 0.100 - 1.00e+18 ohm0.100 - 1.00e+18 ohmAverage value: 2.35e+16 ohm Grade Count:54
Dielectric Constant 1.11 - 62.01.11 - 62.0Average value: 5.66 Grade Count:59
Dielectric Strength 3.00 - 305 kV/mm76.2 - 7760 kV/inAverage value: 35.6 kV/mm Grade Count:54
Dissipation Factor 0.0000400 - 0.3100.0000400 - 0.310Average value: 0.0130 Grade Count:42
Dielectric Loss Index 0.00180 - 0.01060.00180 - 0.0106Average value: 0.00490 Grade Count:5
Comparative Tracking Index 125 - 399 V125 - 399 VAverage value: 197 V Grade Count:21
Hot Wire Ignition, HWI 30.0 - 120 sec30.0 - 120 secAverage value: 67.5 sec Grade Count:6
High Amp Arc Ignition, HAI 0.000 - 15.0 arcs0.000 - 15.0 arcsAverage value: 7.50 arcs Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.30 - 72.0 µm/m-°C2.39 - 40.0 µin/in-°FAverage value: 41.4 µm/m-°C Grade Count:85
 0.234 - 144 µm/m-°C
@Temperature 15.6 - 400 °C
0.130 - 80.0 µin/in-°F
@Temperature 60.0 - 752 °F
Average value: 46.9 µm/m-°C Grade Count:60
CTE, linear, Transverse to Flow 4.70 - 55.0 µm/m-°C2.61 - 30.6 µin/in-°FAverage value: 47.1 µm/m-°C Grade Count:32
 36.0 - 70.0 µm/m-°C
@Temperature 50.0 - 300 °C
20.0 - 38.9 µin/in-°F
@Temperature 122 - 572 °F
Average value: 52.2 µm/m-°C Grade Count:8
Specific Heat Capacity 0.925 - 1.24 J/g-°C0.221 - 0.296 BTU/lb-°FAverage value: 1.04 J/g-°C Grade Count:24
 0.895376 - 1.42256 J/g-°C
@Temperature 60.0 - 300 °C
0.214000 - 0.340000 BTU/lb-°F
@Temperature 140 - 572 °F
Average value: 1.12 J/g-°C Grade Count:5
Thermal Conductivity 0.0330 - 4.47 W/m-K0.229 - 31.0 BTU-in/hr-ft²-°FAverage value: 0.721 W/m-K Grade Count:75
 0.220 - 2.05 W/m-K
@Temperature 40.0 - 300 °C
1.53 - 14.2 BTU-in/hr-ft²-°F
@Temperature 104 - 572 °F
Average value: 0.595 W/m-K Grade Count:16
Melting Point 247 - 388 °C477 - 730 °FAverage value: 379 °C Grade Count:16
Maximum Service Temperature, Air 200 - 395 °C392 - 743 °FAverage value: 287 °C Grade Count:64
Hot Ball Pressure Test 125 °C257 °FAverage value: 125 °C Grade Count:12
Deflection Temperature at 0.46 MPa (66 psi) 215 - 377 °C419 - 711 °FAverage value: 282 °C Grade Count:44
Deflection Temperature at 1.8 MPa (264 psi) 196 - 470 °C385 - 878 °FAverage value: 271 °C Grade Count:88
Vicat Softening Point 221 - 260 °C430 - 500 °FAverage value: 241 °C Grade Count:18
Minimum Service Temperature, Air -240 - -20.0 °C-400 - -4.00 °FAverage value: -193 °C Grade Count:15
Glass Transition Temp, Tg -20.0 - 397 °C-4.00 - 747 °FAverage value: 310 °C Grade Count:82
Decomposition Temperature 431 - 570 °C808 - 1060 °FAverage value: 489 °C Grade Count:4
UL RTI, Electrical 50.0 - 160 °C122 - 320 °FAverage value: 123 °C Grade Count:11
UL RTI, Mechanical with Impact 50.0 - 130 °C122 - 266 °FAverage value: 110 °C Grade Count:11
UL RTI, Mechanical without Impact 50.0 - 160 °C122 - 320 °FAverage value: 123 °C Grade Count:11
Flammability, UL94 V-0 - 5VAV-0 - 5VAGrade Count:73
Flame Spread Index 0.000 - 5.000.000 - 5.00Average value: 1.60 Grade Count:3
Oxygen Index 30.0 - 53.0 %30.0 - 53.0 %Average value: 45.8 % Grade Count:27
Glow Wire Test 850 - 960 °C1560 - 1760 °FAverage value: 905 °C Grade Count:12
 
Optical PropertiesMetricEnglishComments
Haze 0.100 - 2.00 %0.100 - 2.00 %Average value: 1.69 % Grade Count:11
Transmission, Visible 58.0 - 91.6 %58.0 - 91.6 %Average value: 61.6 % Grade Count:11
 
Processing PropertiesMetricEnglishComments
Processing Temperature 371 - 420 °C700 - 788 °FAverage value: 399 °C Grade Count:14
Nozzle Temperature 375 - 405 °C707 - 761 °FAverage value: 388 °C Grade Count:18
Melt Temperature 370 - 416 °C698 - 780 °FAverage value: 393 °C Grade Count:29
Mold Temperature 135 - 232 °C275 - 450 °FAverage value: 180 °C Grade Count:35
Drying Temperature 150 - 204 °C302 - 400 °FAverage value: 173 °C Grade Count:29
Moisture Content 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:11
Dew Point -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:11
Injection Pressure 138 - 193 MPa20000 - 28000 psiAverage value: 165 MPa Grade Count:17
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 inAverage value: 0.00505 cm Grade Count:18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyimide, Unfilled
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyimide, Thermoset Film

O4200 / 77781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.