MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyimide, Thermoset Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 - 2.08 g/cc0.0502 - 0.0751 lb/in³Average value: 1.46 g/cc Grade Count:54
Water Absorption 0.200 - 3.00 %0.200 - 3.00 %Average value: 2.27 % Grade Count:42
Moisture Absorption at Equilibrium 0.400 - 2.50 %0.400 - 2.50 %Average value: 1.57 % Grade Count:14
Water Vapor Transmission 2.40 - 17.5 g/m²/day0.155 - 1.13 g/100 in²/dayAverage value: 5.88 g/m²/day Grade Count:8
 1.70 - 1.70 g/m²/day
@Temperature 38.0 - 38.0 °C
0.109 - 0.109 g/100 in²/day
@Temperature 100 - 100 °F
Average value: 1.70 g/m²/day Grade Count:1
 1.70 - 1.70 g/m²/day
@Time 86400 - 86400 sec
0.109 - 0.109 g/100 in²/day
@Time 24.0 - 24.0 hour
Average value: 1.70 g/m²/day Grade Count:1
Oxygen Transmission 9.90 cc-mm/m²-24hr-atm25.1 cc-mil/100 in²-24hr-atmAverage value: 9.90 cc-mm/m²-24hr-atm Grade Count:5
Viscosity 5000 - 110000 cP
@Temperature 30.0 - 30.0 °C
5000 - 110000 cP
@Temperature 86.0 - 86.0 °F
Average value: 38700 cP Grade Count:3
Thickness 0.102 - 3180 microns0.00400 - 125 milAverage value: 378 microns Grade Count:78
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 5.93 - 540 MPa860 - 78300 psiAverage value: 207 MPa Grade Count:35
 290 - 290 MPa
@Temperature 300 - 300 °C
42100 - 42100 psi
@Temperature 572 - 572 °F
Average value: 290 MPa Grade Count:1
Film Tensile Strength at Yield, MD 49.0 - 255 MPa7110 - 37000 psiAverage value: 123 MPa Grade Count:27
 36.0 - 43.0 MPa
@Temperature 200 - 200 °C
5220 - 6240 psi
@Temperature 392 - 392 °F
Average value: 40.3 MPa Grade Count:3
Film Tensile Strength at Yield, TD 100 - 160 MPa14500 - 23200 psiAverage value: 130 MPa Grade Count:17
Tensile Strength, Yield 73.3 - 160 MPa10600 - 23200 psiAverage value: 128 MPa Grade Count:4
Film Elongation at Break, MD 10.0 - 85.0 %10.0 - 85.0 %Average value: 67.4 % Grade Count:39
Film Elongation at Yield, MD 40.0 - 50.0 %40.0 - 50.0 %Average value: 45.4 % Grade Count:14
Film Elongation at Yield, TD 45.0 - 55.0 %45.0 - 55.0 %Average value: 47.9 % Grade Count:14
Elongation at Break 1.50 - 160 %1.50 - 160 %Average value: 53.2 % Grade Count:44
 70.0 - 70.0 %
@Temperature 300 - 300 °C
70.0 - 70.0 %
@Temperature 572 - 572 °F
Average value: 70.0 % Grade Count:1
Elongation at Yield 10.0 - 110 %10.0 - 110 %Average value: 53.4 % Grade Count:9
Modulus of Elasticity 0.0410 - 10.8 GPa5.95 - 1570 ksiAverage value: 5.49 GPa Grade Count:22
 3.70 - 3.70 GPa
@Temperature 300 - 300 °C
537 - 537 ksi
@Temperature 572 - 572 °F
Average value: 3.70 GPa Grade Count:1
Poissons Ratio 0.3400.340Average value: 0.340 Grade Count:31
Shear Strength 4.30922 - 24.4764 MPa
@Temperature -55.0 - 391 °C
625.001 - 3550.01 psi
@Temperature -67.0 - 736 °F
Average value: 11.9 MPa Grade Count:1
 4.48159 - 16.4095 MPa
@Temperature 260 - 371 °C
650.001 - 2380.00 psi
@Temperature 500 - 700 °F
Average value: 11.9 MPa Grade Count:1
 4.48159 - 16.4095 MPa
@Time 270000 - 7.20e+6 sec
650.001 - 2380.00 psi
@Time 75.0 - 2000 hour
Average value: 11.9 MPa Grade Count:1
Adhesive Bond Strength 0.172 - 0.461 MPa25.0 - 66.9 psiAverage value: 0.351 MPa Grade Count:5
Secant Modulus 2.28 - 5.20 GPa331 - 754 ksiAverage value: 3.04 GPa Grade Count:34
 1.14 - 1.62 GPa
@Temperature 200 - 200 °C
165 - 235 ksi
@Temperature 392 - 392 °F
Average value: 1.38 GPa Grade Count:3
Secant Modulus, MD 1.76 - 9.12 GPa256 - 1320 ksiAverage value: 5.34 GPa Grade Count:3
Coefficient of Friction 0.400 - 0.4800.400 - 0.480Average value: 0.475 Grade Count:33
Coefficient of Friction, Static 0.6300.630Average value: 0.630 Grade Count:31
Tear Strength Test 7.20 - 4307.20 - 430Average value: 108 Grade Count:6
Tear Strength 1.78 - 17.4 kN/m10.2 - 99.5 pliAverage value: 6.21 kN/m Grade Count:10
Peel Strength 0.0880 - 0.280 kN/m0.502 - 1.60 pliAverage value: 0.237 kN/m Grade Count:14
Elmendorf Tear Strength MD 8.20 - 270 g8.20 - 270 gAverage value: 96.1 g Grade Count:4
Film Tensile Strength at Break, MD 98.1 - 736 MPa14200 - 107000 psiAverage value: 248 MPa Grade Count:40
Film Tensile Strength at Break, TD 98.1 - 175 MPa14200 - 25400 psiAverage value: 136 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 2.30e+17 ohm-cm1.00e+9 - 2.30e+17 ohm-cmAverage value: 4.19e+16 ohm-cm Grade Count:68
 1.00e+15 - 1.00e+16 ohm-cm
@Temperature 200 - 200 °C
1.00e+15 - 1.00e+16 ohm-cm
@Temperature 392 - 392 °F
Average value: 4.00e+15 ohm-cm Grade Count:3
Surface Resistance 1.00 - 1.00e+17 ohm1.00 - 1.00e+17 ohmAverage value: 4.99e+15 ohm Grade Count:36
 1.00e+15 - 1.00e+15 ohm
@Temperature 200 - 200 °C
1.00e+15 - 1.00e+15 ohm
@Temperature 392 - 392 °F
Average value: 1.00e+15 ohm Grade Count:2
Dielectric Constant 2.40 - 4.002.40 - 4.00Average value: 3.47 Grade Count:49
 3.20 - 3.30
@Temperature 200 - 200 °C
3.20 - 3.30
@Temperature 392 - 392 °F
Average value: 3.25 Grade Count:2
 3.20 - 3.30
@Frequency 1000 - 1000 Hz
3.20 - 3.30
@Frequency 1000 - 1000 Hz
Average value: 3.25 Grade Count:2
Dielectric Strength 6.70 - 433 kV/mm170 - 11000 kV/inAverage value: 178 kV/mm Grade Count:84
 48.0 - 272 kV/mm
@Temperature 200 - 200 °C
1220 - 6910 kV/in
@Temperature 392 - 392 °F
Average value: 157 kV/mm Grade Count:3
Dissipation Factor 0.00130 - 0.01000.00130 - 0.0100Average value: 0.00351 Grade Count:43
 0.00560 - 0.00780
@Temperature 200 - 200 °C
0.00560 - 0.00780
@Temperature 392 - 392 °F
Average value: 0.00670 Grade Count:2
 0.00560 - 0.00780
@Frequency 1000 - 1000 Hz
0.00560 - 0.00780
@Frequency 1000 - 1000 Hz
Average value: 0.00670 Grade Count:2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.000 - 220 µm/m-°C0.000 - 122 µin/in-°FAverage value: 30.3 µm/m-°C Grade Count:41
 3.00 - 40.0 µm/m-°C
@Temperature 50.0 - 300 °C
1.67 - 22.2 µin/in-°F
@Temperature 122 - 572 °F
Average value: 34.5 µm/m-°C Grade Count:34
 27.0 - 68.0 µm/m-°C
@Temperature 125 - 175 °C
15.0 - 37.8 µin/in-°F
@Temperature 257 - 347 °F
Average value: 34.5 µm/m-°C Grade Count:5
 27.0 - 68.0 µm/m-°C
@Thickness 1.00 - 1.00 mm
15.0 - 37.8 µin/in-°F
@Thickness 0.0394 - 0.0394 in
Average value: 34.5 µm/m-°C Grade Count:5
Specific Heat Capacity 1.09 - 1.15 J/g-°C0.261 - 0.275 BTU/lb-°FAverage value: 1.10 J/g-°C Grade Count:40
Thermal Conductivity 0.120 - 0.500 W/m-K0.833 - 3.47 BTU-in/hr-ft²-°FAverage value: 0.157 W/m-K Grade Count:40
Maximum Service Temperature, Air 180 - 400 °C356 - 752 °FAverage value: 359 °C Grade Count:45
Maximum Service Temperature, Inert 155 - 400 °C311 - 752 °FAverage value: 299 °C Grade Count:18
Minimum Service Temperature, Air -269 - -250 °C-452 - -418 °FAverage value: -268 °C Grade Count:32
Glass Transition Temp, Tg 26.0 - 500 °C78.8 - 932 °FAverage value: 340 °C Grade Count:50
Decomposition Temperature 550 - 584 °C1020 - 1080 °FAverage value: 563 °C Grade Count:5
Flammability, UL94 V-0V-0Grade Count:62
Oxygen Index 37.0 - 66.0 %37.0 - 66.0 %Average value: 50.8 % Grade Count:8
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45 - 1.701.45 - 1.70Average value: 1.67 Grade Count:38
Transmission, Visible 0.000 - 88.0 %0.000 - 88.0 %Average value: 18.6 % Grade Count:8
UV Transmittance 50.0 %50.0 %Average value: 50.0 % Grade Count:6
Emissivity (0-1) 0.450 - 0.7700.450 - 0.770Average value: 0.620 Grade Count:3
Reflection Coefficient, Visible (0-1) 0.0500 - 0.7400.0500 - 0.740Average value: 0.251 Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyimide
Overview of materials for Thermoplastic Polyimide, Unfilled
DuPont™ Kapton® KJ Polyimide Film
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products

O4251 / 78308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.