MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Kendall® C915 Fifth Wheel Grease NLGI Grade 1
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Kendall® C-915 Fifth Wheel Grease is a smooth-textured calcium grease specially developed to handle the severe loads associated with fifth wheel applications. C-915 Fifth Wheel Grease is manufactured with a high-viscosity base oil, a calcium stearate soap thickener and 10% graphite. It provides high load-carrying capacity for protection against wear, and is specially formulated to repel water and resist washout.

Applications:

  • Truck fifth wheels
  • Mobile and industrial equipment operating at mild temperatures and under heavy loads
Features/Benefits:
  • High load-carrying capacity
  • Excellent resistance to water washout

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.901 g/cc0.0326 lb/in³
Viscosity Measurement 9595Index
Saybolt Viscosity at 100°F 2320 SUS2320 SUS
Saybolt Viscosity at 210°F 144 SUS144 SUS
Kinematic Viscosity at 40°C (104°F) 434 cSt434 cSt
Kinematic Viscosity at 100°C (212°F) 29.2 cSt29.2 cSt
 
Mechanical PropertiesMetricEnglishComments
Penetration P(60), 1/10 mm 310 - 340310 - 340ASTM D217
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 °C149 °F
Minimum Service Temperature, Air -9.00 °C15.8 °F
Dropping Point 141 °C286 °F
 
Descriptive Properties
ColorBlack
Graphite0.1
ThickenerCalcium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Triton® XD5 NGLI Grade 1
Phillips 66 Triton® OSP 320 NLGI Grade 2
Phillips 66 Omniguard® NLGI Grade 1
Phillips 66 Omniguard® 460 NLGI Grade 1
Lubriplate SYN LUBE 22 PAO-Based Multi-Purpose Synthetic Fluid

WCON5323 / 198576

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.