MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Finathene® HL 328 HDPE resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusion

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D 792
Water Vapor Transmission 10.86 g/m²/day0.6994 g/100 in²/dayE 96/66
Thickness 25.4 microns1.00 mil
Melt Flow 0.28 g/10 min
@Load 2.16 kg
0.28 g/10 min
@Load 4.76 lb
ASTM D 1238
High Load Melt Index 20 g/10 min
@Load 21.6 kg
20 g/10 min
@Load 47.6 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 24.1 MPa3500 psiASTM D 882 A
Film Tensile Strength at Yield, TD 24.1 MPa3500 psiASTM D 882 A
Film Elongation at Break, MD 600 %600 %ASTM D 882 A
Film Elongation at Break, TD 700 %700 %ASTM D 882 A
Elmendorf Tear Strength MD 50 g50 gASTM D 1922
Elmendorf Tear Strength TD 500 g500 gASTM D 1992
Dart Drop Test 130 g0.287 lbASTM D 1709 A
Film Tensile Strength at Break, MD >= 40.7 MPa>= 5900 psiASTM D 882A
Film Tensile Strength at Break, TD >= 34.5 MPa>= 5000 psiASTM D 882 A
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °FASTM D3417

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer
Borealis Borstar® FB1350 Medium Density Polyethylene
DuPont Fusabond® MX110D Linear Low Density Polyethylene
ICO Polymers ICORENE™ 110-1080 LMDPE Rotational Molding Resin
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded

PFINAP099 / 38682

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.