MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Hot Punch Compound H
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Texaco Hot Punch Compound H is a dark, semi-fluid calcium soap thickened grease designed for use as a die lubricant. It contains graphite and telc, which enhance its lubricity.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 221979; MSDS Number: 9020

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 43 %43 %
Saybolt Viscosity at 100°F 3775 SUS3775 SUSSee Note 1.
Saybolt Viscosity at 210°F 148 SUS148 SUSSee Note 1.
Kinematic Viscosity at 40°C (104°F) 685 cSt685 cStSee Note 1.
Kinematic Viscosity at 100°C (212°F) 30 cSt30 cStSee Note 1.
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 415415Unworked, 25°C (77°F)
 
Thermal PropertiesMetricEnglishComments
Flash Point 260 °C500 °FSee Note 1.
 
Descriptive Properties
ColorBlack
TextureSmooth
Thickener, %1.5Calcium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Centak Centak 11 Extreme Pressure Gear Lubricant
NeoGraf GRAFOIL® TG679 Expanded Natural Graphite Powder

WTEXA246 / 77125

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.