MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Americas Styrenics Styron® 692 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Product Characteristics:
  • High tensile strength
  • High stiffness
  • Food Contact Compliant
  • UL Classification 94 HB
Typical Applications:
  • Appliance parts
  • Housewares

Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM Data
Linear Mold Shrinkage 0.00400 - 0.00800 cm/cm0.00400 - 0.00800 in/in
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 109109
Tensile Strength at Break 47.0 MPa6820 psiASTM D638
Tensile Strength 46.9 MPa6800 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 3.10 GPa450 ksiASTM D638
Flexural Strength 59.3 MPa8600 psiASTM D790
Flexural Modulus 3.34 GPa485 ksiASTM D790
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 °C
27.8 µin/in-°F
@Temperature 73.4 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 187 °C369 °FUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FUnannealed; ASTM Data
Vicat Softening Point 210 °C410 °F
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 213 - 243 °C415 - 469 °FInjection Molding
Zone 1 177 - 193 °C351 - 379 °FExtrusion Molding
 218 - 249 °C424 - 480 °FInjection Molding
Zone 2 182 - 204 °C360 - 399 °FExtrusion Molding
 218 - 249 °C424 - 480 °FInjection Molding
Zone 3 188 - 210 °C370 - 410 °FExtrusion Molding
 199 - 213 °C390 - 415 °FInjection Molding
Zone 4 199 - 216 °C390 - 421 °FExtrusion Molding
Zone 5 204 - 221 °C399 - 430 °FExtrusion Molding
Die Temperature 199 - 232 °C390 - 450 °FExtrusion Molding
Melt Temperature 193 - 232 °C379 - 450 °FExtrusion Molding
Back Pressure 25.0 - 175 MPa3630 - 25400 psiInjection Molding
 
Descriptive Properties
Head Pressure10-21 MPa
Melt Pump, Adapter, Pipes, Screen Changer193-232°C
Polish Rolls66-104°C
Zone # 6204-221°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDW174_a / 323915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.