MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wieland Simidur S 2 PFM Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Material Notes: Palladium-base ceramic alloy

Applications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneering

Dental

Key Words: EN ISO 9693
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.2 g/cc0.405 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 410410HV5/30; after porcelain firing
 450450HV5/30; hardened
Tensile Strength, Yield  909.76 MPa
@Strain 0.2 %
131950 psi
@Strain 0.2 %
after porcelain firing
 989.74 MPa
@Strain 0.2 %
143550 psi
@Strain 0.2 %
hardened
Elongation at Break 2.0 %2.0 %hardened
 4.0 %4.0 %after porcelain firing
Modulus of Elasticity 122 GPa17700 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.2 µm/m-°C
@Temperature 25.0 - 500 °C
7.89 µin/in-°F
@Temperature 77.0 - 932 °F
Melting Point 1100 - 1190 °C2010 - 2170 °F
Solidus 1100 °C2010 °F
Liquidus 1190 °C2170 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 849 °C1560 °FPreheating Temp.
Casting Temperature 1340 °C2440 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 9.5 %9.5 %
Gallium, Ga 9.0 %9.0 %
Germanium, Ge 0.50 %0.50 %
Gold, Au 2.0 %2.0 %
Palladium, Pd 79 %79 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Palladium Alloy
Overview of materials for Refractory Metal
Niobium FS-85 (Nb-28Ta-10W-1Zr), Recrystallized
Niobium C-103 (WC 103; 89Nb-10Hf-1Ti), Cold-Rolled
NAECO® ELKONIUM® 43 palladium based alloy

NWIELAN16 / 19818

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.