MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes: DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a variety of applications primarily on submarines. This advanced acetal material uses a combination of PTFE fibers uniformly dispersed in Delrin acetal resin. The combination results in improved wear characteristics along with strength, toughness, dimensional stability and machinability. The profile also yields a material with superior load bearing capabilities, especially when operating at high speeds.
  • Developed specifically for US Naval use
  • Meets requirements for NAVSEA 5959311 rev C and NAVSEA 803-4384678 rev B and C
  • Meets requirements per General dynamics Dwg. 4384678 rev C note 7 with Drn C2
  • All stock shapes are traceable to resin lot and batch
DELRIN® DE588 is designed and approved specifically for naval applications and is suitable in a variety of uses such as bushings, bearings, seals, gaskets and valve seats.

Information provided by Ensinger

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115
Tensile Strength, Yield 42.1 MPa6100 psiASTM D638
Elongation at Yield 20 %20 %ASTM D638
Tensile Modulus 2.21 GPa320 ksiASTM D638
 2.50 GPa363 ksiinjection molded samples; ASTM D638
Compressive Strength  14.5 MPa
@Strain 1 %
2100 psi
@Strain 1 %
ASTM D695
 75.8 MPa
@Strain 10 %
11000 psi
@Strain 10 %
ASTM D695
Izod Impact, Notched 0.587 J/cm1.10 ft-lb/inASTM D256
Tensile Impact Strength 10.5 kJ/m²5.00 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 175 °C347 °FASTM D3418
Maximum Service Temperature, Air 85.0 °C185 °Flong term
 149 °C300 °Fintermittent
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
Delrin Delrin® 100AF POM-PTFE20
Mitsubishi Chemical Advanced Materials Acetron™ AF Blend / Ertacetal™ H-TF POM-H PTFE-filled, extruded
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM)
Ensinger Delrin® 150 Homopolymer Acetal (POM)

PENSIN095 / 122205

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.