MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Omniguard® NLGI Grade 1
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Omniguard is a high-performance, multipurpose, extreme pressure (EP), corrosion-preventive grease specially developed for use in industrial and automotive equipment operating in wet or corrosive environments. It is particularly recommended for equipment exposed to water contamination, saltwater corrosion and/or high temperatures. Omniguard is manufactured with high-quality base oils and a non-soap, calcium sulfonate thickener. It is fortified with antiwear additives and rust and corrosion inhibitors. It protects against rust and corrosion in high-humidity, high-temperature applications such as those found in the steel, lumber, tire manufacturing and paper industries. It has excellent load-carrying capacity, high shear stability and outstanding resistance to water washout. Omniguard Grade No. 2 is NLGI GC-LB certified for use as a multipurpose automotive wheel bearing and chassis lubricant

Applications:

  • Industrial and automotive equipment operating at high temperatures and exposed to water contamination, high humidity or corrosive environmental conditions
  • Marine equipment, heavy mobile equipment and cables exposed to salt water
  • Paper machine wet- and dry-end bearings and hot calendar stacks
  • Rolling mills, hot roll tables, continuous casters, ingot buggies and slab mills
  • Steel mill roller bearings, conveyors and gears
  • Centralized lube systems and auto lubbers in service shops
Features/Benefit:
  • Excellent oxidation resistance and thermal stability at high temperatures
  • Outstanding rust and corrosion protection, including resistance to saltwater corrosion
  • Excellent extreme-pressure and antiwear properties
  • Outstanding resistance to water washout
  • Excellent shear stability
  • High dropping point (>550°F)
  • Light-colored, low staining
  • NLGI GC-LB certified (Grade No. 2)

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.993 g/cc0.0359 lb/in³
Viscosity Measurement 9696Index
Saybolt Viscosity at 100°F 1160 SUS1160 SUS
Saybolt Viscosity at 210°F 96 SUS96 SUS
Kinematic Viscosity at 40°C (104°F) 219 cSt219 cSt
Kinematic Viscosity at 100°C (212°F) 18.8 cSt18.8 cSt
Oxidative Stability 100 hour
@Pressure 0.000 MPa
100 hour
@Pressure 0.000 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 500 kg1100 lb (mass)ASTM D2596
Four Ball Wear 0.390 mm0.0154 inScar Diameter; ASTM D2266
Penetration 310 - 340310 - 340
Timken Test 29500 g65.0 lbOK Load; ASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -29.0 °C-20.2 °F
Dropping Point 300 °C572 °F
 
Descriptive Properties
ColorTan
Roll Stability0.07Change in Penetration, ASTM D1831
Shear Stability0.01Change (100,000 strokes), ASTM D217
ThickenerCalcium Sulfonate
Water Washout Resistance2.81Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Triton® XD5 NGLI Grade 1
Phillips 66 Triton® OSP 320 NLGI Grade 2
Phillips 66 Omniguard® 460 NLGI Grade 1
Phillips 66 Kendall® C915 Fifth Wheel Grease NLGI Grade 1
Lubriplate SYN LUBE 22 PAO-Based Multi-Purpose Synthetic Fluid

WCON5130 / 198383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.