MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 8103-14 One-Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting; Potting; Encapsulating; Embedding applications where 2-component systems can not be used; Electronic and structural components, patterns, and medical equipment; Coating; Impregnation; Resurfacing; Insulation; Bonding metal, ceramics, glass, and most rigid materials; Assembly; Patching; and Filling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 200 cP200 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888
Tensile Strength at Break 57.9 MPa8400 psi
Elongation at Break 5.1 %5.1 %
Flexural Strength 83.4 MPa12100 psi
Flexural Modulus 2.28 GPa330 ksi
Compressive Strength 75.2 MPa10900 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.04e+14 ohm-cm3.04e+14 ohm-cmC 96/23/96
 3.80e+15 ohm-cm3.80e+15 ohm-cm"A"
Surface Resistance 1.13e+14 ohm1.13e+14 ohmC 96/23/96
 3.93e+15 ohm3.93e+15 ohmCond. A
Dielectric Constant  3.12
@Frequency 1e+6 Hz
3.12
@Frequency 1e+6 Hz
A
 3.26
@Frequency 60 Hz
3.26
@Frequency 60 Hz
A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 79.0 °C174 °FDeflection Temp at unknown load
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 150 - 160 °C
1.00 - 2.00 hour
@Temperature 302 - 320 °F
 60.0 - 240 min
@Temperature 160 - 180 °C
1.00 - 4.00 hour
@Temperature 320 - 356 °F
optional
Pot Life 205 min
@Temperature 100 °C
205 min
@Temperature 212 °F
Shelf Life 5.00 - 8.00 Month5.00 - 8.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® Stycast® 933-48 One-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® 926-82-1 One-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® 906-1 One-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® E-1030 One-Component Epoxy Low Stress Encapsulant
Trelleborg Emerson & Cuming Stycast® E-1000 One-Component Epoxy Low Stress Encapsulant

PABC822 / 107806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.