MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Grade 702 Zirconium, Commercially Pure
Categories: Metal; Nonferrous Metal; Zirconium Alloy; Pure Element

Material Notes: Characteristics:
  • Ductile
  • Mechanical Properties similar to titanium and austenitic stainless steel
  • Excellent corrosion resistance
  • Forms stable oxide layer
  • Highly anisotropic

Applications: Chemical processing equipment

Machining Parameters: Use slow speeds, heavy feeds and flood cooling with a water-soluble oil lubricant

Key Words: UNS R60702, Zircadyne® 702
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.50 g/cc0.235 lb/in³
Vapor Pressure  0.0000133 bar
@Temperature 2000 °C
0.0100 torr
@Temperature 3630 °F
 1.20 bar
@Temperature 3600 °C
900 torr
@Temperature 6510 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 4949Estimated from Vickers
Hardness, Rockwell B 7878Estimated from Vickers
Hardness, Vickers 150150Annealed Sample
Tensile Strength, Ultimate >= 379 MPa>= 55000 psi
 140 MPa
@Temperature 400 °C
20300 psi
@Temperature 752 °F
 205 MPa
@Temperature 300 °C
29700 psi
@Temperature 572 °F
 230 MPa
@Temperature 200 °C
33400 psi
@Temperature 392 °F
 350 MPa
@Temperature 100 °C
50800 psi
@Temperature 212 °F
 450 MPa
@Temperature 20.0 °C
65300 psi
@Temperature 68.0 °F
Tensile Strength, Yield  80.0 MPa
@Temperature 400 °C
11600 psi
@Temperature 752 °F
 90.0 MPa
@Temperature 300 °C
13100 psi
@Temperature 572 °F
 150 MPa
@Temperature 200 °C
21800 psi
@Temperature 392 °F
 260 MPa
@Temperature 100 °C
37700 psi
@Temperature 212 °F
 325 MPa
@Temperature 20.0 °C
47100 psi
@Temperature 68.0 °F
 >= 207 MPa
@Strain 0.2 %
>= 30000 psi
@Strain 0.2 %
Elongation at Break 16 %16 %in 50 mm
 21 %
@Temperature 400 °C
21 %
@Temperature 752 °F
 32 %
@Temperature 20.0 °C
32 %
@Temperature 68.0 °F
 38 %
@Temperature 100 °C
38 %
@Temperature 212 °F
 50 %
@Temperature 300 °C
50 %
@Temperature 572 °F
 56 %
@Temperature 230 °C
56 %
@Temperature 446 °F
Modulus of Elasticity 99.3 GPa14400 ksi
Poissons Ratio 0.350.35
Fatigue Strength  60.0 MPa
@# of Cycles 3.00e+7
8700 psi
@# of Cycles 3.00e+7
notched
 125 MPa
@# of Cycles 500000
18100 psi
@# of Cycles 500000
notched
 145 MPa
@# of Cycles 3.00e+7
21000 psi
@# of Cycles 3.00e+7
unnotched
 175 MPa
@# of Cycles 5000
25400 psi
@# of Cycles 5000
unnotched
Shear Modulus 36.2 GPa5250 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000397 ohm-cm0.0000397 ohm-cmTemp Coefficient is 0.0044/°C at 20°C
Magnetic Susceptibility 0.000001340.00000134cgs/g; pure Zr
Critical Magnetic Field Strength, Oersted 4747Pure Zr
Critical Superconducting Temperature 0.595 - 0.625 K0.595 - 0.625 Kpure Zr
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 250 J/g108 BTU/lb
Heat of Vaporization 6490 J/g2790 BTU/lb
CTE, linear  5.89 µm/m-°C
@Temperature 25.0 °C
3.27 µin/in-°F
@Temperature 77.0 °F
 6.30 µm/m-°C
@Temperature 250 °C
3.50 µin/in-°F
@Temperature 482 °F
 6.90 µm/m-°C
@Temperature 500 °C
3.83 µin/in-°F
@Temperature 932 °F
Specific Heat Capacity 0.285 J/g-°C0.0681 BTU/lb-°F
Thermal Conductivity 22.0 W/m-K153 BTU-in/hr-ft²-°F
Melting Point 1852 °C3366 °F
Boiling Point 4377 °C7911 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.320.32650 nm; unoxidized pure Zr sample; total
 
Component Elements PropertiesMetricEnglishComments
Fe + Cr 0.20 %0.20 %
Hafnium, Hf <= 4.5 %<= 4.5 %
Oxygen, O 0.16 %0.16 %
Zirconium, Zr >= 99.2 %>= 99.2 %includes Hf
 
Descriptive Properties
Alpha Phase Crystal Structurehcp< 865°C
Beta Phase Crystal Structurebcc> 865°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Grade 705 Zirconium (Zr-2.5Nb)
Zircaloy-4 Zirconium Alloy
Reactor Grade Zirconium
Zirconium, Zr
Zr-2.5Nb Zirconium Alloy, Nuclear Grade

MZRI00 / 14570

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.