MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use where severe temperature conditions exist.

SILTEX 36 is manufactured to a finished weight of 36 ounces per square yard. It's heavier weight and tight 12-harness satin weave makes SILTEX 36 the premium product for maximum protection of personnel and equipment against more severe welding splatter, sparks, grinding of metals, etc. SILTEX 36 is also excellent for use in engineered thermal insulation systems that requiring higher strength and improved thermal properties over the lighter-weight materials.

The amorphous silica fibers that make up SILTEX are unaffected by most chemicals, except strong alkalis, hydrofluoric acid or sodium.

All SILTEX fabrics are available in standard “C” and pre-shrunk (fired) versions, Fabrics are available with several coating/treatment options that enhance certain properties of the product in order to meet required performance characteristics.

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³Calculated from weight of 36 oz/sy
Thickness 1270 microns50.0 milnom
 
Thermal PropertiesMetricEnglishComments
Melting Point 1700 °C3100 °F
Maximum Service Temperature, Air 982 °C1800 °FContinuous
 1260 °C2300 °FIntermittent use
Shrinkage 8.0 - 12 %
@Temperature 982 °C
8.0 - 12 %
@Temperature 1800 °F
Linear
 <= 3.0 %
@Temperature 704 °C,
Time 1800 sec
<= 3.0 %
@Temperature 1300 °F,
Time 0.500 hour
Linear
 
Descriptive Properties
Break StrengthMin 270 x 180 lbnom, warp x fill (1" x 4")
ConstructionWoven fabric, 12 harness satin weave
MaterialAmorphous Silica 96-99%
Packaging50 ly per roll or 150 ly master roll
Tolerance10%
Width, standard36 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon
Covestro Makrolon® 2558 Polycarbonate
Honeywell Spectra® 1000 Fiber
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
Honeywell Spectra® S--900 650-926 Fiber

CMID06 / 1510

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.