MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Triton® XD5 NGLI Grade 1
Categories: Fluid; Lubricant; Calcium Gellant; Polyalphaolefin (PAO)

Material Notes: Triton XD5 is a premium quality, synthetic, extreme-pressure (EP) calcium sulfonate grease developed for use in off-road equipment operating at moderate to very low temperatures. It is particularly recommended for use in mobile equipment such as haul trucks, backhoes, excavators, front-end loaders and motor graders operating in wet conditions and under heavy loads. Triton XD5 is manufactured with a low-viscosity, synthetic polyalphaolefin (PAO) base oil and a non-soap, calcium sulfonate thickener. It is compounded with select additives to provide excellent oxidation resistance, extreme-pressure and antiwear properties, and protection against rust and corrosion. It is fortified with 5% molybdenum disulfide (moly) for extra wear protection under conditions involving heavy or shock loading. The low-viscosity synthetic base oil provides outstanding pumpability at low temperatures. Triton XD5 has a distinctive platinum color for identification.

Applications:

  • Off-road construction and mining equipment operating at moderate to very low temperatures
  • Steering linkages, kingbolt bearings, pin joints, universal joints and other articulated pivots
  • Heavily loaded plain and rolling-element bearings in off-road equipment
  • Conveyor and fan bearings in chemical and manufacturing plants that require a corrosion-resistant grease with moly
  • Centralized lube systems
Features/Benefits:
  • High load-carrying capacity
  • Excellent wear protection
  • Contains 5% moly for extra protection against galling and wear under shock loads
  • Outstanding low-temperature properties
  • Excellent resistance to water washout
  • Protects against rust and corrosion

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.893 g/cc0.0323 lb/in³
Viscosity Measurement 117117Index
Saybolt Viscosity at 100°F 180 SUS180 SUS
Saybolt Viscosity at 210°F 46 SUS46 SUS
Kinematic Viscosity at 40°C (104°F) 35 cSt35 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt6.0 cSt
Oxidative Stability 100 hour
@Pressure 0.0207 MPa
100 hour
@Pressure 3.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 800 kg1760 lb (mass)ASTM D2596
Four Ball Wear <= 0.450 mm<= 0.0177 inScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 310 - 340310 - 340ASTM D217
Timken Test 29500 g65.0 lbOK Load; ASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
Dropping Point >= 288 °C>= 550 °F
 
Descriptive Properties
ColorPlatinum
Composition5%Molybdenum Disulfide
Copper Corrosion1aASTM D4048
ThickenerCalcium Sulfonate
Water Washout Resistance0.02Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Triton® OSP 320 NLGI Grade 2
Phillips 66 Omniguard® NLGI Grade 1
Phillips 66 Omniguard® 460 NLGI Grade 1
Phillips 66 Kendall® C915 Fifth Wheel Grease NLGI Grade 1
Lubriplate SYN LUBE 22 PAO-Based Multi-Purpose Synthetic Fluid

WCON5150 / 198403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.