System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
AISI 1030 Steel, annealed at 845°C (1550°F)
AISI 1030 Steel, annealed at 845°C (1550°F), furnace cooled 11°C (20°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
AISI 1030 Steel, as rolled
AISI 1030 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1030 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1030 Steel, normalized 925°C (1700°F)
AISI 1030 Steel, normalized at 925°C (1700°F), air cooled, 100 mm (4 in.) round
AISI 1030 Steel, normalized at 925°C (1700°F), air cooled, 13 mm (0.5 in.) round
AISI 1030 Steel, normalized at 925°C (1700°F), air cooled, 25 mm (1 in.) round
AISI 1030 Steel, normalized at 925°C (1700°F), air cooled, 50 mm (2 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 650°C (1200°F) temper, 100 mm (4 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 650°C (1200°F) temper, 50 mm (2 in.) round
AISI 1034 Steel
AISI 1035 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
AISI 1035 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
AISI 1035 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
AISI 1035 Steel, as cold drawn, 50-75 mm (2-3 in) round
AISI 1035 Steel, as rolled, 19-32 mm (0.75-1.25 in) round
AISI 1035 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1035 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1035 Steel, cold drawn, high temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1035 Steel, cold drawn, high temperature, stress relieved, 32-50 mm (1.25-2 in) round
AISI 1035 Steel, cold drawn, high temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1035 Steel, cold drawn, low temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1035 Steel, cold drawn, low temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1035 Steel, cold drawn, low temperature, stress relieved, 32-50 mm (1.25-2 in) round
AISI 1035 Steel, cold drawn, low temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1035 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1035 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper
AISI 1037 Steel, Cold Drawn Bar (UNS G10370)
AISI 1037 Steel, Hot Rolled Bar (UNS G10370)
AISI 1038 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1038 Steel, hot rolled round, 19-32 mm (0.75-1.25 in)
AISI 1038H Steel
AISI 1039 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1039 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1040 Steel, annealed at 790°C (1450°F)
AISI 1040 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
AISI 1040 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
AISI 1040 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
AISI 1040 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
AISI 1040 Steel, as cold drawn, 50-75 mm (2-3 in) round
AISI 1040 Steel, as rolled
AISI 1040 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1040 Steel, cold drawn, high temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1040 Steel, cold drawn, high temperature, stress relieved, 32-50 mm (1.25-2 in) round
AISI 1040 Steel, cold drawn, high temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1040 Steel, cold drawn, low temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1040 Steel, cold drawn, low temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1040 Steel, cold drawn, low temperature, stress relieved, 32-50 mm (1.25-2 in) round
AISI 1040 Steel, cold drawn, low temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1040 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1040 Steel, normalized at 900°C (1650°F)
AISI 1040 Steel, normalized at 900°C (1650°F), air cooled, 100 mm (4 in.) round
AISI 1040 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round
AISI 1040 Steel, normalized at 900°C (1650°F), air cooled, 25 mm (1 in.) round
AISI 1040 Steel, normalized at 900°C (1650°F), air cooled, 50 mm (2 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 650°C (1200°F) temper, 100 mm (4 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 1040 Steel, oil quenched from 855°C (1570°F), 650°C (1200°F) temper, 50 mm (2 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 1040 Steel, water quenched from 845°C (1550°F), 650°C (1200°F) temper, 50 mm (2 in.) round
AISI 1042 Steel, Cold Drawn Bar (UNS G10420)
AISI 1042 Steel, Hot Rolled Bar (UNS G10420)
AISI 1042 Steel, Normalized Cold Drawn Bar (UNS G10420)
AISI 1043 Steel, Cold Drawn Bar (UNS G10430)
AISI 1043 Steel, Hot Rolled Bar (UNS G10430)
AISI 1043 Steel, Normalized Cold Drawn Bar (UNS G10430)
AISI 1044 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1044 Steel, merchant quality, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
AISI 1045 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
AISI 1045 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
AISI 1045 Steel, as cold drawn, 50-75 mm (2-3 in) round
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, cold drawn, high temperature stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1045 Steel, cold drawn, high temperature stress relieved, 32-50 mm (1.25-2 in) round
AISI 1045 Steel, cold drawn, high temperature stress relieved, 50-75 mm (2-3 in) round
AISI 1045 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1045 Steel, cold drawn, low temperature, stress relieved round (16 - 22 mm)
AISI 1045 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, Quenched and Tempered to 390 HB
AISI 1045 Steel, Quenched and Tempered to 450 HB
AISI 1045 Steel, Quenched and Tempered to 500 HB
AISI 1045 Steel, Quenched and Tempered to 595 HB
AISI 1045 Steel, turned, ground, and polished, 19-32 mm (0.75-1.25 in) round
AISI 1046 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1046 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1046 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1049 Steel, Annealed Cold Drawn Bar (UNS G10490)
AISI 1049 Steel, Cold Drawn Bar (UNS G10490)
AISI 1049 Steel, Hot Rolled Bar (UNS G10490)
AISI 1050 Steel, annealed at 790°C (1450°F)
AISI 1050 Steel, annealed at 790°C (1450°F), furnace cooled 10°C (18°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
AISI 1050 Steel, as cold drawn bar, 16-22 mm (0.625-0.875 in) round
AISI 1050 Steel, as cold drawn bar, 22-32 mm (0.875-1.25 in) round
AISI 1050 Steel, as cold drawn bar, 32-50 mm (1.25-2 in) round
AISI 1050 Steel, as cold drawn bar, 50-75 mm (2-3 in) round
AISI 1050 Steel, as rolled
AISI 1050 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1050 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1050 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1050 Steel, cold drawn, high temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1050 Steel, cold drawn, high temperature, stress relieved, 32-50 mm (1.25-2 in) round
AISI 1050 Steel, cold drawn, high temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1050 Steel, cold drawn, low temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1050 Steel, cold drawn, low temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1050 Steel, cold drawn, low temperature, stress relieved, 32-50 mm (1.25-2 in) round
AISI 1050 Steel, cold drawn, low temperature, stress relieved, 50-75 mm (2-3 in) round
AISI 1050 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1050 Steel, normalized at 900°C (1650°F)
AISI 1050 Steel, normalized at 900°C (1650°F), air cooled, 100 mm (4 in.) round
AISI 1050 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round
AISI 1050 Steel, normalized at 900°C (1650°F), air cooled, 25 mm (1 in.) round
AISI 1050 Steel, normalized at 900°C (1650°F), air cooled, 50 mm (2 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 1050 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 50 mm (2 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 650°C (1200°F) temper, 100 mm (4 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 1050 Steel, water quenched from 830°C (1525°F), 650°C (1200°F) temper, 50 mm (2 in.) round
AISI 1053 Steel Composition Spec (UNS G10530)
AISI 1055 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1055 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1059 Steel
AISI 1060 Steel, annealed at 790°C (1450°F)
AISI 1060 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
AISI 1060 Steel, as rolled
AISI 1060 Steel, cold drawn, spheroidized annealed, 19-32 mm (0.75-1.25 in) round
AISI 1060 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1060 Steel, normalized at 900°C (1650°F)
AISI 1060 Steel, normalized at 900°C (1650°F), air cooled, 100 mm (4 in.) round
AISI 1060 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round
AISI 1060 Steel, normalized at 900°C (1650°F), air cooled, 25 mm (1 in.) round
AISI 1060 Steel, normalized at 900°C (1650°F), air cooled, 50 mm (2 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 480°C (900°F) temper, 100 mm (4 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 480°C (900°F) temper, 13 mm (0.5 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 480°C (900°F) temper, 25 mm (1 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 480°C (900°F) temper, 50 mm (2 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 1064 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1064 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1065 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1065 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1069 Steel Composition Spec (UNS G10690)
AISI 1070 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1070 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1074 Steel, cold drawn, spheroidized, annealed (discontinued)
AISI 1074 Steel, cold rolled strip (discontinued)
AISI 1074 Steel, hot rolled, (discontinued)
AISI 1075 Carbon Steel Bar
AISI 1078 Steel, Hot Rolled Bar (UNS G10780)
AISI 1078 Steel, Spheroidized Annealed and Cold Drawn Bar (UNS G10780)
AISI 1080 Steel, annealed at 790°C (1450°F)
AISI 1080 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
AISI 1080 Steel, as rolled
AISI 1080 Steel, cold drawn, spheroidized annealed, 19-32 mm (0.75-1.25 in) round
AISI 1080 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1080 Steel, normalized at 900°C (1650°F), air cooled, 100 mm (4 in.) round
AISI 1080 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round
AISI 1080 Steel, normalized at 900°C (1650°F), air cooled, 25 mm (1 in.) round
AISI 1080 Steel, normalized at 900°C (1650°F), air cooled, 50 mm (2 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 480°C (900°F) temper, 100 mm (4 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 480°C (900°F) temper, 25 mm (1 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 480°C (900°F) temper, 50 mm (2 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 595°C (1100°F) temper
AISI 1080 Steel, oil quenched from 815°C (1500°F), 595°C (1100°F) temper, 100 mm (4 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), 595°C (1100°F) temper, 50 mm (2 in.) round
AISI 1080 Steel, oil quenched from 815°C (1500°F), tempered at 480°C (900°F)
AISI 1080 Steel, oil quenched from 815°C (1500°F), tempered at 540°C (1000°F)
AISI 1084 Steel, Hot Rolled Bar (UNS G10840)
AISI 1084 Steel, Spheroidized Annealed and Cold Drawn Bar (UNS G10840)
AISI 1085 Carbon Steel, Hot Rolled Bar
AISI 1085 Carbon Steel, Spheroidized Annealed and Cold Drawn Bar
AISI 1086 Steel, Hot Rolled Bar (UNS G10860)
AISI 1086 Steel, Spheroidized Annealed and Cold Drawn Bar (UNS G10860)
AISI 1090 Steel, cold drawn, spheroidized annealed, 19-32 mm (0.75-1.25 in) round
AISI 1090 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1095 Steel, annealed at 790°C (1450°F)
AISI 1095 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
AISI 1095 Steel, as rolled
AISI 1095 Steel, cold drawn, spheroidized annealed, 19-32 mm (0.75-1.25 in) round
AISI 1095 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1095 Steel, normalized at 900°C (1650°F)
AISI 1095 Steel, normalized at 900°C (1650°F), air cooled, 100 mm (4 in.) round
AISI 1095 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round
AISI 1095 Steel, normalized at 900°C (1650°F), air cooled, 25 mm (1 in.) round
AISI 1095 Steel, normalized at 900°C (1650°F), air cooled, 50 mm (2 in.) round
AISI 1095 Steel, oil quenched 800°C (1470°F), 480°C (900°F) temper, 100 mm (4 in.) round
AISI 1095 Steel, oil quenched 800°C (1470°F), 480°C (900°F) temper, 25 mm (1 in.) round
AISI 1095 Steel, oil quenched 800°C (1470°F), 480°C (900°F) temper, 50 mm (2 in.) round
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.