System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
LyondellBasell Koattro PB M 8510M Polybutene Random Copolymer
LyondellBasell Koattro PB M 8911M Polybutene Random Copolymer
LyondellBasell LH735200 HDPE
LyondellBasell Lucalen A2540D Low Density Polyethylene
LyondellBasell Lucalen A2700H Low Density Polyethylene
LyondellBasell Lucalen A2700M Low Density Polyethylene
LyondellBasell Lucalen A2700P LDPE
LyondellBasell Lucalen A2910M Low Density Polyethylene
LyondellBasell Lucalen A2920M Low Density Polyethylene
LyondellBasell Lucalen G3710E Anhydride-Modified Polyethylene
LyondellBasell Luflexen hyPE 35P FA Polyethylene
LyondellBasell Luflexen hyPE 36R FA Polyethylene
LyondellBasell Luflexen hyPE 52R FA HDPE
LyondellBasell Luflexen hyPE 56P FA HDPE
LyondellBasell Lupolen 1800 H LDPE, Injection Molding Grade
LyondellBasell Lupolen 1800 S LDPE, Injection Molding Grade
LyondellBasell Lupolen 1800H Low Density Polyethylene (LDPE), Blow Molding Grade
LyondellBasell Lupolen 1800P Polyethylene
LyondellBasell Lupolen 1800S Polyethylene
LyondellBasell Lupolen 1800U Polyethylene
LyondellBasell Lupolen 1804 H LDPE, Film Grade
LyondellBasell Lupolen 1810 D LDPE
LyondellBasell Lupolen 1810 E LDPE
LyondellBasell Lupolen 1810 H LDPE, Injection Molding Grade
LyondellBasell Lupolen 1812 D LDPE
LyondellBasell Lupolen 1812 E LDPE
LyondellBasell Lupolen 1840 D LDPE, Film Grade
LyondellBasell Lupolen 1840 H LDPE
LyondellBasell Lupolen 1840D Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 1842 D SW 413 LDPE
LyondellBasell Lupolen 1852 H SW 413 LDPE
LyondellBasell Lupolen 2003 H LDPE, Film Grade
LyondellBasell Lupolen 2012 D SW 413 LDPE
LyondellBasell Lupolen 2210 H SK LDPE
LyondellBasell Lupolen 2220H LDPE
LyondellBasell Lupolen 2221D LDPE
LyondellBasell Lupolen 2221F LDPE
LyondellBasell Lupolen 2227K LDPE
LyondellBasell Lupolen 2410 T LDPE, Injection Molding Grade
LyondellBasell Lupolen 2420 F LDPE
LyondellBasell Lupolen 2420 H LDPE, Film Grade
LyondellBasell Lupolen 2420 K LDPE, Film Grade
LyondellBasell Lupolen 2420D Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 2420F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 2420F PLUS Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 2420H Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2420K Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2421D LDPE
LyondellBasell Lupolen 2421F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 2421H Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2421K Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2424 H LDPE, Film Grade
LyondellBasell Lupolen 2425 K LDPE, Film Grade
LyondellBasell Lupolen 2426 F LDPE, Film Grade
LyondellBasell Lupolen 2426F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 2426H Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2426K Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2427F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 2427H Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2427K Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2441 D LDPE, Film Grade
LyondellBasell Lupolen 2452 D SW 413 LDPE
LyondellBasell Lupolen 3010 K LDPE, Injection Molding Grade
LyondellBasell Lupolen 3010D Low Density Polyethylene (LDPE), Blow Molding Grade
LyondellBasell Lupolen 3020 D LDPE
LyondellBasell Lupolen 3020 F LDPE
LyondellBasell Lupolen 3020 H LDPE, Film Grade
LyondellBasell Lupolen 3020 K LDPE, Film Grade
LyondellBasell Lupolen 3020F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 3020H Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 3020K Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 3024 H LDPE, Film Grade
LyondellBasell Lupolen 3025 K LDPE, Film Grade
LyondellBasell Lupolen 3026 F LDPE, Film Grade
LyondellBasell Lupolen 3026F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 3026H Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 3026K Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 3032 D LDPE
LyondellBasell Lupolen 3040 D LDPE, Film Grade
LyondellBasell Lupolen 3220 K LDPE, Film Grade
LyondellBasell Lupolen 3220F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 3226 K LDPE, Film Grade
LyondellBasell Lupolen 3412 D LDPE
LyondellBasell Lupolen 3420J Low Density Polyethylene (LDPE), Blow Molding Grade
LyondellBasell Lupolen 3426J Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 3621 M RM Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
LyondellBasell Lupolen 3652 D SW 00413 MDPE
LyondellBasell Lupolen 3721C High Density Polyethylene (HDPE), Blown Film Grade
LyondellBasell Lupolen 3821 D MDPE
LyondellBasell Lupolen 3822 D GB 00350 MDPE
LyondellBasell Lupolen 4021 K RM High Density Polyethylene (HDPE), Rotational Molding Grade
LyondellBasell Lupolen 4152 D SW 00413 HDPE
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade
LyondellBasell Lupolen 4261 A IM High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen 4261A IMBD High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen 4261A Q135 High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261A Q149 High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261A Q416 High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 4261A SW 63200 High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG BD High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
LyondellBasell Lupolen 4261AG Q469 High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG Q474 High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen 4261AG UV High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG UV60005 High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4532D High Density Polyethylene, Steel Pipe Coating Grade
LyondellBasell Lupolen 4552D BLACK High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 5021 D HDPE, Blow Molding Grade
LyondellBasell Lupolen 5021DX High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 5031 L HDPE, Injection Molding Grade
LyondellBasell Lupolen 5031L Q449 K High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5121 A High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 5231 HX HDPE, Impact Grade
LyondellBasell Lupolen 5236 HX HDPE, Impact Grade
LyondellBasell Lupolen 5261 Z HDPE, Blow Molding Grade
LyondellBasell Lupolen 5261 Z HI HDPE
LyondellBasell Lupolen 5261 Z Q 456 B High Density Polyethylene, Pipe and Sheet Extrusion Grade
LyondellBasell Lupolen 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade
LyondellBasell Lupolen 5261 ZS HDPE, Blow Molding Grade
LyondellBasell Lupolen 5261Z HI High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 5261Z High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 5261Z Q456 B High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5261Z Q456 B POWDER High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5261Z Q456 High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5261Z Q456 POWDER High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5261ZS High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 5361 A HDPE, Blow Molding Grade
LyondellBasell Lupolen 5461 B Q 471NA POWDER High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5461B Q471 B High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5461B Q471 High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Lupolen 5621 D HDPE
LyondellBasell Lupolen 6021 D HDPE, Blow Molding Grade
LyondellBasell Lupolen 6031 M HDPE, Injection Molding Grade
LyondellBasell Lupolen GX 4087 Low Density Polyethylene
LyondellBasell Lupolen GX 5038 High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen UHM 201 MDPE, Ultra-High Molecular Weight
LyondellBasell Lupolen UHM 301 MDPE, Ultra-High Molecular Weight
LyondellBasell Lupolen UHM 5000 Ultra High Molecular Weight Polyethylene
LyondellBasell Lupolen V 2520 J Ethylene Vinyl Acetate, Film Grade
LyondellBasell Lupolen V 2920 K Ethylene Vinyl Acetate, lnjection Molding Grade
LyondellBasell Lupolen V 3510 K Ethylene Vinyl Acetate, lnjection Molding Grade
LyondellBasell Lupolen V 3520 K Ethylene Vinyl Acetate
LyondellBasell Lupolex FA LLDPE
LyondellBasell Metocene HM2089 Polypropylene
LyondellBasell Metocene HM562S Polypropylene
LyondellBasell Metocene HM648T Polypropylene, Homopolymer
LyondellBasell Metocene MF650W Polypropylene
LyondellBasell Metocene MF650X Polypropylene
LyondellBasell Metocene MF650Y Polypropylene
LyondellBasell Microthene MN70100 Polyolefin
LyondellBasell Microthene MN71020 Polyolefin
LyondellBasell Microthene MN71120 Polyolefin
LyondellBasell Microthene MN71400 Polyolefin
LyondellBasell Microthene MN72200 Polyolefin
LyondellBasell Microthene MN72700 Polyolefin
LyondellBasell Microthene MP625962 Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
LyondellBasell Microthene MP635962 Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
LyondellBasell Microthene MP643962 Polyethylene
LyondellBasell Microthene MP652962 HDPE
LyondellBasell Microthene MU76000 Polyolefin
LyondellBasell Microthene MU76300 Polyolefin
LyondellBasell Microthene® F FA70000 High Density Polyethylene
LyondellBasell Microthene® F FA70900 High Density Polyethylene
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer
LyondellBasell Microthene® F FN50100 Low Density Polyethylene
LyondellBasell Microthene® F FN51000 Low Density Polyethylene
LyondellBasell Microthene® F FN51900 Low Density Polyethylene
LyondellBasell Microthene® G MN70100 Low Density Polyethylene
LyondellBasell Microthene® G MN71020 Low Density Polyethylene
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding)
LyondellBasell Microthene® G MN71400 Low Density Polyethylene
LyondellBasell Microthene® G MN72200 Low Density Polyethylene
LyondellBasell Microthene® G MN72700 Low Density Polyethylene
LyondellBasell Microthene® G MU76000 Ethylene Vinyl Acetate Copolymer
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP564189X01 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP574189X01 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP675662 Linear Low Density Polyethylene
LyondellBasell Montell 0300 Polybutene
LyondellBasell Montell 0800 Polybutene
LyondellBasell Montell 12C01G2 Clarity LLDPE
LyondellBasell Montell 12C01G3 Clarity LLDPE
LyondellBasell Montell 12C01G4 Clarity LLDPE
LyondellBasell Montell 12C01G5 Clarity LLDPE
LyondellBasell Montell 16501F3 Butene LLDPE
LyondellBasell Montell 16501F4 Butene LLDPE
LyondellBasell Montell 16501F6 Butene LLDPE
LyondellBasell Montell 16501F7 Butene LLDPE
LyondellBasell Montell 16501F8 Butene LLDPE
LyondellBasell Montell 16502F3 Butene LLDPE
LyondellBasell Montell 16502F7 Butene LLDPE
LyondellBasell Montell 16502F8 Butene LLDPE
LyondellBasell Montell 1900 UHMW Polyethylene
LyondellBasell Montell 1900CM UHMW Polyethylene
LyondellBasell Montell 1900H UHMW Polyethylene
LyondellBasell Montell 1900LCM UHMW Polyethylene
LyondellBasell Montell 8340 Polybutene-1
LyondellBasell Montell 8640 Polybutene-1
LyondellBasell Montell HB312CM UHMW Polyethylene
LyondellBasell Montell HB320CM UHMW Polyethylene
LyondellBasell Montell SE191 Polypropylene Impact Copolymer
LyondellBasell Moplen 2000HEXP Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen BA238A Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen CA012/1 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen COAT EP/60 BIANCO Polypropylene Copolymer
LyondellBasell Moplen COAT EP/60 M BIANCO Polypropylene Copolymer
LyondellBasell Moplen EF300K Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EF300N Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP/60 Bianco Polypropylene Copolymer
LyondellBasell Moplen EP1006 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP140R Polypropylene, Impact Copolymer
LyondellBasell Moplen EP200R Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP220R Polypropylene, Extrusion Grade
LyondellBasell Moplen EP222D Polypropylene, Impact Copolymer
LyondellBasell Moplen EP229R Polypropylene, Extrusion Grade
LyondellBasell Moplen EP229S Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP240H Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP240P Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP240T Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP243R Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP249R Polypropylene, Impact Copolymer
LyondellBasell Moplen EP2596 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP2641 Polypropylene, Impact Copolymer
LyondellBasell Moplen EP2838 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP2967 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300C Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300H B Polypropylene, Impact Copolymer
LyondellBasell Moplen EP300H Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300K Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300M Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300N Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300R B Polypropylene, Impact Copolymer
LyondellBasell Moplen EP300R Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300U Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP3046 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP310D HP Polypropylene, Impact Copolymer
LyondellBasell Moplen EP310D Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP310DC Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP310J HP Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP310M HP Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP310RM Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP3201 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP3202 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP3307 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP332C Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP332K Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP332L Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP336J Polypropylene, Impact Modified; Molded/Extruded
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.