MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Thallium, Tl
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.85 g/cc0.4281 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 204.3833204.38331995
Atomic Number 8181
Thermal Neutron Cross Section 3.4 barns/atom3.4 barns/atom
X-ray Absorption Edge 0.1447 Å0.1447 ÅK
 0.80787 Å0.80787 ÅLI
 0.84355 Å0.84355 ÅLII
 0.97968 Å0.97968 ÅLIII
Electrode Potential -0.336 V-0.336 V
Electronegativity 1.81.8Pauling
Ionic Radius 0.950 Å0.950 ÅCrystal Ionic Radius for Valence +3
 1.47 Å1.47 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 2.5 g/A/h2.5 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 2.02.0
Hardness, Vickers 2.02.0
Tensile Strength, Ultimate 7.50 MPa1090 psi
Elongation at Break 40 %40 %in 125 mm
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000150 ohm-cm0.0000150 ohm-cm
Magnetic Susceptibility -2.40e-7-2.40e-7cgs/g
Critical Magnetic Field Strength, Oersted 176 - 180176 - 180
Critical Superconducting Temperature 2.36 - 2.40 K2.36 - 2.40 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 20.9 J/g8.99 BTU/lb
Heat of Vaporization 1231 J/g529.6 BTU/lb
CTE, linear 28.0 µm/m-°C
@Temperature 20.0 - 100 °C
15.6 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.136 J/g-°C0.0325 BTU/lb-°F
Thermal Conductivity 39.4 W/m-K273 BTU-in/hr-ft²-°F
Melting Point 304 °C579 °F
Boiling Point 1473 °C2683 °F
 
Component Elements PropertiesMetricEnglishComments
Thallium, Tl 100 %100 %
 
Descriptive Properties
CAS Number7440-28-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thorium, Th
Titanium, Ti
Osmium, Os; Annealed
Rhenium, Re; Annealed
Thulium, Tm

AMETl00 / 116

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.