MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Description

Polytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temperatures. TPP 503 is UV stable, paintable and pigmentable.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm0.0090 - 0.011 in/in
Melt Index of Compound 9.0 g/10 min9.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Yield 13.8 MPa2000 psiASTM D638
Elongation at Break 600 %600 %ASTM D638
Flexural Modulus 0.310 GPa45.0 ksiASTM D790
Gardner Impact 36.0 J
@Temperature -30.0 °C
26.6 ft-lb
@Temperature -22.0 °F
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -50.0 °C-58.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
LyondellBasell Pro-fax™ SG899 Polypropylene Copolymer
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
A. Schulman DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic

PASHU288 / 25252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.