MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NatureWorks® Ingeo™ 3051D Injection Grade PLA  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: PLA (polylactide) polymer 3051D is designed for injection molding applications where the requirements are clarity with heat deflection temperatures lower than 130ºF (55ºC). Applications include cutlery, cups, plates and saucers, and outdoor novelties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Viscosity Measurement 3.0 - 3.53.0 - 3.5Relative Viscosity
Linear Mold Shrinkage 0.003 - 0.005 cm/cm0.003 - 0.005 in/in
Melt Flow 10 - 25 g/10 min
@Load 2.16 kg,
Temperature 210 °C
10 - 25 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 48.0 MPa6960 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 3.83 GPa556 ksiASTM D790
Izod Impact, Notched 0.160 J/cm0.300 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 - 165 °C302 - 329 °FASTM D3418
Glass Transition Temp, Tg 55.0 - 65.0 °C131 - 149 °FASTM D3417
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Thickness Unknown
 
Processing PropertiesMetricEnglishComments
Feed Temperature 165 °C329 °F
Nozzle Temperature 205 °C401 °F
Melt Temperature 200 °C392 °F
Mold Temperature 25.0 °C77.0 °F
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Screw Speed 100 - 175 rpm100 - 175 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 3001D Injection Grade PLA
NatureWorks® Ingeo™ 3251D Injection Grade PLA
NatureWorks® Ingeo™ 3801X Injection Grade PLA
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer

PNATU82 / 103480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.