MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LD 3127.BR Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: ExxonMobil™ LD 3127.BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: 1000 ppm
  • Slip: 750 ppm
  • Thermal Stabilizer: Yes
Applications:
  • Blend Partner
  • Bread Bags
  • Cast Film
  • Co-Extrusion Films
  • Display Packaging Film
  • Food packaging
  • Form Fill and Seal Packaging
  • High Clarity Film
  • Laundry Film
  • Light Duty Shrink Film
  • Mail Bag
  • Overwrap Film
  • Produce Bags
  • Salad Bags

Information provided by ExxonMobil

Key Words: LDPE LD 144BR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ExxonMobil method
Melt Flow 3.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1000 ppm1000 ppm
Slip Level 750 ppm750 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.1 MPa1900 psiASTM D882
Film Tensile Strength at Yield, TD 11.7 MPa1700 psiASTM D882
Film Elongation at Break, MD 190 %190 %ASTM D882
Film Elongation at Break, TD 470 %470 %ASTM D882
Elmendorf Tear Strength MD 350 g350 gASTM D1922
Elmendorf Tear Strength TD 130 g130 gASTM D1922
Dart Drop Test 60.0 g0.132 lbASTM D1709A
Film Tensile Strength at Break, MD 24.8 MPa3600 psiASTM D882
Film Tensile Strength at Break, TD 17.2 MPa2500 psiASTM D882
1% Secant Modulus, MD 255 MPa37000 psiASTM D882
1% Secant Modulus, TD 303 MPa44000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 6.2 %6.2 %ASTM D1003
Gloss 72 %72 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ Flow m 0527.MC Film Grade Hexene LLDPE
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
ExxonMobil LL 1001XKI Film Grade Butene LLDPE
ExxonMobil LD 2025.BR Low Density Polyethylene Resin
ExxonMobil Exceed™ Flow m 0535.MC Blown Film Grade Hexene LLDPE

PEX99256 / 175492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.