MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exceed™ Flow m 0535.MC Blown Film Grade Hexene LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Exceed™ Flow m 0535.MC Blown resins are ethylene 1-hexene copolymers.  This polymer offers an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior draw down and enhanced toughness.  TnPP is not intentionally added to Enable™3505 MC.   

Availability:   Africa & Middle East, Europe, North America, Asia Pacific, Latin America.  

Additive:  antiblock: no; slip: no; processing aid: yes; thermal stabilizer: yes. 

Applications:  food packaging, multilayer packaging film, shrink film, form fill and seal packaging, stand up pouches, heavy duty bags, lamination film, food packaging.

Information provided by ExxonMobil.

Key Words: Enable™ 3505MC Blown
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³ASTM D1505
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 16.5 MPa2400 psiASTM D882
Film Tensile Strength at Yield, TD 19.3 MPa2800 psiASTM D882
Film Elongation at Break, MD 550 %550 %ASTM D882
Film Elongation at Break, TD 790 %790 %ASTM D882
Puncture Energy 2.26 J1.67 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 20 g20 gASTM D1922
Elmendorf Tear Strength TD 610 g610 gASTM D1922
Dart Drop Test 70.0 g0.154 lbASTM D1709A
Film Tensile Strength at Break, MD 57.9 MPa8400 psiASTM D882
Film Tensile Strength at Break, TD 46.2 MPa6700 psiASTM D882
1% Secant Modulus, MD 427 MPa62000 psiASTM D882
1% Secant Modulus, TD 517 MPa75000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FPeak; ExxonMobil Method
Vicat Softening Point 119 °C246 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %ASTM D1003
Gloss 40 %40 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Baystar™ Lumicene® mPE M 2710 EP Metallocene Medium Density Polyethylene Film Resin
ExxonMobil Exceed™ Flow m 0527.MC Film Grade Hexene LLDPE
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin

PEX98843 / 238227

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.