MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nordel® IP 4520 Molded Golf Grip
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4520 is an amorphous EPDM grade designed for molded applications. It is ideally suited for injection and transfer molded brake parts, corner moldings, general purpose gaskets and moldings. The combination of low viscosity and low crystallinity allows for good processability, low temperature properties and performance without the addition of a plasticizer.

Information provided by manufacturer.

Key Words: 0822A32-01
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.057 g/cc0.03819 lb/in³
Mooney Viscosity 33
@Temperature 100 °C
33
@Temperature 212 °F
ML 1 + 4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 13.5 MPa1960 psiVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 685 %685 %Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 1.60 MPa
@Strain 100 %
232 psi
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 2.70 MPa
@Strain 200 %
392 psi
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 3.80 MPa
@Strain 300 %
551 psi
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 29.5 kN/m168 pliDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 95 %
@Temperature 125 °C
95 %
@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -45.0 °C-49.0 °FTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested1.25TMTD
 1.5ZnDBC
 1.5Sulfur
 100Nordel® IP 4520
 2.5MBT
 20N-650 Black
 3Zinc Oxide
 45Precipitated Silica
 55Paraffinic Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 4640 General Purpose Compound
Dow Nordel® IP 4570 Radiator/Heater Hose
Dow Nordel® IP 4640 Molded Golf Grips
Dow Nordel® IP 4520 General Purpose Molding
Dow Nordel® IP 4760P Compound

PDVG09 / 34129

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.