MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nordel® IP 4570 Radiator/Heater Hose
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4570 is an amorphous EPDM grade designed for extruded applications. It is ideally suited for dense extruded profiles, coolant hose and general purpose moldings. The combination of high viscosity and low crystallinity allows for good balance of processability, extensibility, low-temperature properties and performance.

Information provided by manufacturer.

Key Words: 0625A22-02
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³
Mooney Viscosity 64
@Temperature 100 °C
64
@Temperature 212 °F
ML 1 + 4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 9.30 MPa1350 psiVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 425 %425 %Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 3.30 MPa
@Strain 100 %
479 psi
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 7.90 MPa
@Strain 300 %
1150 psi
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 37.1 kN/m212 pliDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 75 %
@Temperature 100 °C
75 %
@Temperature 212 °F
Pellets cured MDR TC95 + 15 min at 160°C, 22 hr at 100°C; Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -43.0 °C-45.4 °FTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested0.75DPTT
 0.75TMTD
 1Stearic Acid
 1Sulfur
 1ZnDBC
 1.5MBTS
 100Nordel® IP 4570
 100Paraffinic Oil
 160N-650 Black
 30Ground Calcium Carbonate
 5Zinc Oxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 4770P Highly Extended Low-Cost Hose
Dow Nordel® IP 4520 General Purpose Compound
Dow Nordel® IP 4640 General Purpose Compound
Dow Nordel® IP 4770R Highly Extended Low-Cost Hose
Dow Nordel® IP 4520 General Purpose Molding

PDVG16 / 34136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.