MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nordel® IP 4770R Highly Extended Low-Cost Hose
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4770R is a high molecular weight semicrystalline grade and offers fast cure rates and high states of cure with standard sulfur cure systems. It offers high green strength and high extensibility. It is designed for extruded applications such as profiles and hose. It is also suitable for molded goods. This grade is available in rod form for improved mixing speed and throughput.

Information provided by manufacturer.

Key Words: 0639A04-06
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.339 g/cc0.04837 lb/in³
Mooney Viscosity 21
@Temperature 100 °C
21
@Temperature 212 °F
ML 1 + 4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6161Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 7.00 MPa1020 psiVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 492 %492 %Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 3.90 MPa
@Strain 200 %
566 psi
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 5.20 MPa
@Strain 300 %
754 psi
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 31.0 kN/m177 pliDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 75 %
@Temperature 125 °C
75 %
@Temperature 257 °F
Pellets cured MDR t'95 + 15 min, 70 hr; Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -15.0 °C5.00 °FTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested1Sulfur
 1ZnDMC
 1TMTD
 1DTDM
 1.5MBTS
 100Nordel® IP 4770R
 125Naphthenic Oil
 2Stearic Acid
 2Paraffin Wax
 2ZnDBC
 200N-650 Black
 200Ground Calcium Carbonate
 5Zinc Oxide
 50N-550 Black
 75Paraffinic Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 4570 Radiator/Heater Hose
Dow Nordel® IP 4770P Highly Extended Low-Cost Hose
Dow Nordel® IP 5565 Dense Extruded Profile
Dow Nordel® IP 4640 Low Cost General Purpose Hose
Dow Nordel® IP 4640 General Purpose Compound

PDVG38 / 34158

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.