MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nordel® IP 4640 Low Cost General Purpose Hose
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4640 is an amorphous EPDM grade designed for molded and extruded applications. It is ideally suited for general-purpose gaskets and moldings, extruded profiles and hoses. The combination of medium viscosity and low crystallinity allows for good balance of processability, low temperature properties and product performance.

Information provided by manufacturer.

Key Words: 0640-03-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.157 g/cc0.04180 lb/in³
Mooney Viscosity 37
@Temperature 100 °C
37
@Temperature 212 °F
ML 1 + 4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6464Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 7.20 MPa1040 psiVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 423 %423 %Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 2.60 MPa
@Strain 100 %
377 psi
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 5.20 MPa
@Strain 200 %
754 psi
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 6.40 MPa
@Strain 300 %
928 psi
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 29.6 kN/m169 pliDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 64 %
@Temperature 125 °C
64 %
@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -36.0 °C-32.8 °FTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested0.5Sulfur
 1TETD
 1Tetrone® A
 1TMTD
 1TMTM
 1Stearic Acid
 1.5ZnDBC
 100Nordel® IP 4640
 140Naphthenic Oil
 200N-550 Black
 5Parrafin Wax
 5Zinc Oxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Dow Nordel® IP 4770P Highly Extended Low-Cost Hose
Dow Nordel® IP 4570 Radiator/Heater Hose
Dow Nordel® IP 4770R Highly Extended Low-Cost Hose
Dow Nordel® IP 4520 General Purpose Molding

PDVG20 / 34140

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.