MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

European Birch Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Large
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years)
Resistance to penetration by preservatives: Permeable
Common Applications: Plywood, furniture, turnery

Key Words: Betula pubescens; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.730 g/cc0.0264 lb/in³Air Dry (12-15% Moisture Content)
Cell Length 1.40 mm0.0551 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 6.90 MPa1000 psiPerpendicular to Grain
 134 MPa19400 psiAxial
Modulus of Rupture 0.144 GPa20.9 ksiStatic Bending
Flexural Modulus 16.17 GPa2345 ksiStatic Bending
Compressive Strength 10.8 MPa1570 psiPerpendicular to Grain
 50.0 MPa7250 psiParallel to Grain
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 11.8 MPa1710 psiOrientation Unknown
Toughness 33.2 J24.5 ft-lb2 cm x 2 cm sample
Cleavage 5.20 kN/m29.7 lb/in
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.60 %0.60 %Axial; Green to Zero Moisture
 5.3 %5.3 %Radial; Green to Zero Moisture
 7.8 %7.8 %Tangential; Green to Zero Moisture
 14.2 %14.2 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorWhite to light brown Usual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Yellow Birch Wood
Sweet Birch Wood
Paper Birch Wood
American Birch Wood
American Maple, Rock (Sugar Maple)

PTSE040 / 71313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.