MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® 103HSL NC010 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Unreinforced, Heat Stabilized, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Melt Density 0.980 g/cc
@Temperature 290 °C
0.0354 lb/in³
@Temperature 554 °F
Water Absorption 8.5 %
@Thickness 2.00 mm
8.5 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
 1.2 %
@Thickness 3.00 mm,
Time 86400 sec
1.2 %
@Thickness 0.118 in,
Time 24.0 hour
Immersion; DAM; Sim. to ISO 62
Moisture Absorption 2.60 %
@Thickness 2.00 mm
2.60 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number 150 cm³/g1.50 dl/gSulfuric acid 96%; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 85.0 MPa12300 psiH 358/30; 50% RH; ISO 2039-1
 160 MPa23200 psiH 961/30; DAM; ISO 2039-1
 180 MPa26100 psiH 358/30; DAM; ISO 2039-1
Tensile Strength, Yield 55.0 MPa7980 psi50% RH; ISO 527-1/-2
 85.0 MPa12300 psiDAM; ISO 527-1/-2
Elongation at Break 4.5 %4.5 %parallel; DAM; ISO 527-3
 20 %20 %Nominal; DAM; ISO 527-1/-2
 >= 50 %>= 50 %Nominal; 50% RH; ISO 527-1/-2
Elongation at Yield 4.3 %4.3 %DAM; ISO 527-1/-2
 25 %25 %50% RH; ISO 527-1/-2
Tensile Modulus 1.40 GPa203 ksi50% RH; ISO 527-1/-2
 3.10 GPa450 ksiDAM; ISO 527-1/-2
Flexural Strength  65.0 MPa
@Strain 3.5 %
9430 psi
@Strain 3.5 %
50% RH; ISO 178
 95.0 MPa
@Strain 3.5 %
13800 psi
@Strain 3.5 %
DAM; ISO 178
Flexural Modulus 1.30 GPa189 ksiDS; 50% RH; ISO 178
 2.80 GPa406 ksiDS; DAM; ISO 178
Poissons Ratio 0.370.37DAM
 0.430.4350% RH
Izod Impact, Notched (ISO)  3.50 kJ/m²
@Temperature -40.0 °C
1.67 ft-lb/in²
@Temperature -40.0 °F
DS; 50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
DS; DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO)  300 kJ/m²
@Temperature -30.0 °C
143 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 180/1U
Charpy Impact Unnotched  40.0 J/cm²
@Temperature -30.0 °C
190 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.250 J/cm²
@Temperature -40.0 °C
1.19 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.250 J/cm²
@Temperature -40.0 °C
1.19 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.350 J/cm²
@Temperature -30.0 °C
1.67 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.550 J/cm²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 1200 MPa174000 psi1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 650 MPa94300 psi1000h; 50% RH; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm50% RH; IEC 62631-3-1
 1.00e+15 ohm-cm1.00e+15 ohm-cmDAM; IEC 62631-3-1
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
DAM; IEC 62631-2-1
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 12.8
@Frequency 100 Hz
12.8
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 28.0 kV/mm711 kV/in50% RH; IEC 60243-1
 31.0 kV/mm787 kV/inDAM; IEC 60243-1
Dissipation Factor  0.0075
@Frequency 100 Hz
0.0075
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.0165
@Frequency 1e+6 Hz
0.0165
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.070
@Frequency 1e+6 Hz
0.070
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 0.58
@Frequency 100 Hz
0.58
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 >= 600 V
@Thickness 3.00 mm
>= 600 V
@Thickness 0.118 in
PLC 0; DAM; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FDAM; ISO 11359-1/-2
Specific Heat Capacity 2.79 J/g-°C
@Temperature 290 °C
0.667 BTU/lb-°F
@Temperature 554 °F
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 290 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 554 °F
Melt
Melting Point 262 °C504 °F10°C/min; DAM; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °C284 °FTemperature index, Tensile strength 20,000h; DAM; IEC 60216-1
 155 °C311 °FTemperature index, Tensile strength 5000h; DAM; IEC 60216-1
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FDAM; ISO 75-1/-2
Vicat Softening Point 240 °C464 °F50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 40.0 °C104 °F10°C/min; 50% RH; ISO 11357-1/-2
 60.0 °C140 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  V-2
@Thickness 0.710 mm
V-2
@Thickness 0.0280 in
DAM; IEC 60695-11-10
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Oxygen Index 28 %28 %DAM; ISO 4589-1/-2
Glow Wire Test  700 °C
@Thickness 0.750 mm
1290 °F
@Thickness 0.0295 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 1.00 mm
1290 °F
@Thickness 0.0394 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
No Flame; DAM; IEC 60335-1
Glow Wire Ignition Temperature  725 °C
@Thickness 0.750 mm
1340 °F
@Thickness 0.0295 in
DAM; IEC 60695-2-13
 725 °C
@Thickness 1.50 mm
1340 °F
@Thickness 0.0591 in
DAM; IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
1340 °F
@Thickness 0.118 in
DAM; IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °FOptimum, Injection
 280 - 300 °C536 - 572 °FRange, Injection
Mold Temperature 70.0 °C158 °FOptimum, Injection
 50.0 - 90.0 °C122 - 194 °FInjection
Ejection Temperature 190 °C374 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5E-08
Emission of organic compounds (µgC/g)2.1VDA 277
FMVSS ClassSEISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,,M1G1HNR,S14-030
Max. screw tangential speed (m/s)0.4Injection
Odor Class2.5VDA 270
Part Marking Code>PA66<ISO 11469
PolymerPA66
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPA66ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 103HSL BKB080 PA66
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (DAM)
Ravago Manufacturing Americas Hylon N1000EHL Nylon 66
Celanese Zytel® ST801 NC010A PA66-HI
Celanese Zytel® ST801A NC010A PA66-HI

PDSX5303 / 197943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.